Combining wet etching and real-time damage event imaging to reveal the most dangerous laser damage initiator in fused silica
文献类型:期刊论文
作者 | Hu, Guohang; Zhao, Yuanan; Liu, Xiaofeng; Li, Dawei; Xiao, Qiling; Yi, Kui; Shao, Jianda |
刊名 | opt. lett.
![]() |
出版日期 | 2013 |
卷号 | 38期号:15页码:2632 |
通讯作者 | zhao, ya (reprint author), chinese acad sci, shanghai inst opt & fine mech, key lab mat high power laser, shanghai 201800, peoples r china. |
英文摘要 | a reliable method, combining a wet etch process and real-time damage event imaging during a raster scan laser damage test, has been developed to directly determine the most dangerous precursor inducing low-density laser damage at 355 nm in fused silica. it is revealed that similar to 16% of laser damage sites were initiated at the place of the scratches, similar to 49% initiated at the digs, and similar to 35% initiated at invisible defects. the morphologies of dangerous scratches and digs were compared with those of moderate ones. it is found that local sharp variation at the edge, twist, or inside of a subsurface defect is the most dangerous laser damage precursor. (c) 2013 optical society of america |
收录类别 | SCI |
语种 | 英语 |
版本 | 出版稿 |
源URL | [http://ir.siom.ac.cn/handle/181231/14782] ![]() |
专题 | 上海光学精密机械研究所_中科院强激光材料重点实验室 |
作者单位 | 1.[Hu, Guohang 2.Zhao, Yuanan 3.Liu, Xiaofeng 4.Li, Dawei 5.Xiao, Qiling 6.Yi, Kui 7.Shao, Jianda] Chinese Acad Sci, Shanghai Inst Opt & Fine Mech, Key Lab Mat High Power Laser, Shanghai 201800, Peoples R China |
推荐引用方式 GB/T 7714 | Hu, Guohang,Zhao, Yuanan,Liu, Xiaofeng,et al. Combining wet etching and real-time damage event imaging to reveal the most dangerous laser damage initiator in fused silica[J]. opt. lett.,2013,38(15):2632. |
APA | Hu, Guohang.,Zhao, Yuanan.,Liu, Xiaofeng.,Li, Dawei.,Xiao, Qiling.,...&Shao, Jianda.(2013).Combining wet etching and real-time damage event imaging to reveal the most dangerous laser damage initiator in fused silica.opt. lett.,38(15),2632. |
MLA | Hu, Guohang,et al."Combining wet etching and real-time damage event imaging to reveal the most dangerous laser damage initiator in fused silica".opt. lett. 38.15(2013):2632. |
入库方式: OAI收割
来源:上海光学精密机械研究所
浏览0
下载0
收藏0
其他版本
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。