Fracture of colloidal single-crystal films fabricated by controlled vertical drying deposition
文献类型:期刊论文
作者 | Cao H(曹鹤)![]() ![]() ![]() ![]() ![]() ![]() |
刊名 | Physical Review E
![]() |
出版日期 | 2010 |
卷号 | 82期号:3页码:31602 |
通讯作者邮箱 | wangyr@imech.ac.cn |
关键词 | Fine Particles Crack Patterns Forces Dispersions Suspension Contact Latexes Model Gaps |
ISSN号 | 1539-3755 |
通讯作者 | Wang YR |
合作状况 | 国际 |
中文摘要 | Controlled vertical drying deposition method was used to make high-quality single crystal close-packed colloidal films formed of different radii polystyrene latex spheres on glass substrates coming from a low concentration water suspension (0.1% volume fraction). Regardless of the spheres radii the film thickness was about 6.3 microns. However, cracks destroyed the crystalline film structure during the colloidal film growth. The effect of particle radius (85-215 nm range) on film cracking was systematically studied using in situ optical fracture monitoring. Primary parallel cracks run along the vertical growth direction, later followed by secondary branched cracks in-between the primary cracks due to residual water evaporation. Quantitative theoretical relationship between the cracks spacing and particles radius was derived and shows good agreement with experimental observations. Normalized cracks spacing is related to a reciprocal ratio of the dimensionless particle radius. |
类目[WOS] | Physics, Fluids & Plasmas ; Physics, Mathematical |
研究领域[WOS] | Physics |
关键词[WOS] | FINE PARTICLES ; CRACK PATTERNS ; FORCES ; DISPERSIONS ; SUSPENSION ; CONTACT ; LATEXES ; MODEL ; GAPS |
收录类别 | SCI |
资助信息 | National Natural Science Foundation of China [10832011]; Chinese Academy of Sciences [KJCX2-YW-L08]; National Science Foundation [CMMI-0600266] |
原文出处 | http://dx.doi.org/10.1103/PhysRevE.82.031602 |
语种 | 英语 |
WOS记录号 | WOS:000281488400004 |
公开日期 | 2011-03-01 ; 2011-03-30 |
源URL | [http://dspace.imech.ac.cn/handle/311007/43635] ![]() |
专题 | 力学研究所_国家微重力实验室 |
通讯作者 | Wang YR |
推荐引用方式 GB/T 7714 | Cao H,Lan D,Wang YR,et al. Fracture of colloidal single-crystal films fabricated by controlled vertical drying deposition[J]. Physical Review E,2010,82(3):31602. |
APA | 曹鹤.,蓝鼎.,王育人.,Volinsky AA.,段俐.,...&Wang YR.(2010).Fracture of colloidal single-crystal films fabricated by controlled vertical drying deposition.Physical Review E,82(3),31602. |
MLA | 曹鹤,et al."Fracture of colloidal single-crystal films fabricated by controlled vertical drying deposition".Physical Review E 82.3(2010):31602. |
入库方式: OAI收割
来源:力学研究所
浏览0
下载0
收藏0
其他版本
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。