In Vivo Study on Degradation Behavior and Histologic Response of Pure Magnesium in Muscles

文献类型:期刊论文

作者Chen, Shanshan ; Tan, Lili ; Zhang, Bingchun ; Xia, Yonghui ; Xu, Ke ; Yang, Ke
刊名JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY
出版日期2017-05-01
卷号33期号:5页码:469-474
关键词Pure magnesium Degradation behavior Histologic response Muscle tissue
ISSN号1005-0302
通讯作者Yang, K (reprint author), Chinese Acad Sci, Inst Met Res, Shenyang 110016, Peoples R China.
中文摘要When an orthopedics device is implanted into bone injury site, it will contact the soft tissue (skeletal muscle, fascia, ligament etc.) except for bone. Magnesium based biodegradable metals are becoming an important research object in orthopedics due to their bioactivity to promote bone healing. In this study, pure Mg rods with and without chemical conversion coating were implanted into the muscle tissue of rabbits. Implants and their surrounding tissues were taken out for weight loss measurement, cross-sectional scanning electron microscopy observation, elemental distribution analysis and histological examination. The results showed that the chemical conversion coating would increase the in vivo corrosion resistance of pure Mg and decrease the accumulation of calcium (Ca) and phosphorus (P) elements around the implants. For the bare magnesium implant, both Ca and P contents in the surrounding tissues increased at the initial stage of implantation and then decreased at 12 weeks implantation, while for the magnesium with chemical conversion coating, Ca and P contents in the surrounding tissues decreased with the implantation time, but were not significant. The histological results demonstrated that there was no calcification in the muscle tissue with implantation of magnesium for up to 12 weeks. The chemical conversion coating not only increased the in vivo corrosion resistance of pure Mg, but also avoided the depositions of Ca and P in the surrounding tissues, meaning that pure magnesium should be bio-safe when contacting with muscle tissues. Copyright (C) 2017, The editorial office of Journal of Materials Science & Technology. Published by Elsevier Limited.
学科主题Materials Science, Multidisciplinary ; Metallurgy & Metallurgical Engineering
收录类别SCI
资助信息National Science & Technology Pillar Program of China [2012BAl18B01]; National Basic Research Program of China ("973 Program") [2012CB619101]; National Natural Science Foundation of China [81171443]; Foundation of Jiangsu Collaborative Innovation Center of Biomedical Functional Materials
语种英语
公开日期2017-08-17
源URL[http://ir.imr.ac.cn/handle/321006/78151]  
专题金属研究所_中国科学院金属研究所
推荐引用方式
GB/T 7714
Chen, Shanshan,Tan, Lili,Zhang, Bingchun,et al. In Vivo Study on Degradation Behavior and Histologic Response of Pure Magnesium in Muscles[J]. JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY,2017,33(5):469-474.
APA Chen, Shanshan,Tan, Lili,Zhang, Bingchun,Xia, Yonghui,Xu, Ke,&Yang, Ke.(2017).In Vivo Study on Degradation Behavior and Histologic Response of Pure Magnesium in Muscles.JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY,33(5),469-474.
MLA Chen, Shanshan,et al."In Vivo Study on Degradation Behavior and Histologic Response of Pure Magnesium in Muscles".JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY 33.5(2017):469-474.

入库方式: OAI收割

来源:金属研究所

浏览0
下载0
收藏0
其他版本

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。