Strong resistance to hydrogen embrittlement of high-entropy alloy

文献类型:期刊论文

作者Pu Z(蒲卓); Chen Y(陈艳); Dai LH(戴兰宏)
刊名MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING
出版日期2018-10-24
卷号736页码:156-166
关键词High-entropy alloy Hydrogen embrittlement Cryogenic temperature Ductility Deformation microstructure
ISSN号0921-5093
DOI10.1016/j.msea.2018.08.101
英文摘要

The resistance to hydrogen embrittlement (HE) of CrMnFeCoNi high-entropy alloy (HEA) at both room and cryogenic temperatures was examined through tensile experiments on specimens hydrogenated via cathodic electrochemical charging method. Two representative steels, i.e. 316L stainless steel (SS) and X80 pipeline steel (PS), were chosen for comparison due to their similar main constituent elements to CrMnFeCoNi HEA. Results show that the hydrogen pre-charged CrMnFeCoNi HEA has the smallest loss of ductility among the three materials at room temperature, while displays no reduction of elongation at 77 K, compared with the uncharged one. Fracture surfaces at both room and cryogenic temperatures of hydrogen pre-charged CrMnFeCoNi HEA are mainly composed of dimples, indicating ductile fractures, while brittle characteristics occur in pre-charged 316L SS and X80 PS. Typical deformation microstructure of the hydrogen pre-charged CrMnFeCoNi HEA at room temperature is tangled dislocations instead of highly dense dislocation walls (HDDWs) found in the pre-charged 316L SS. At 77 K, more deformation twins are formed in the both materials. Reasons for a higher resistance to HE of CrMnFeCoNi HEA at room temperature are attributed to the formation of less hydrogen trapping sites, thus a lower degree of hydrogen enrichment than 316L SS. While at 77 K, the atomic hydrogen is not able to promptly accumulate near these trapping sites due to its slow diffusion rate, which leads to strong HE resistance.

分类号一类
URL标识查看原文
WOS关键词AUSTENITIC STAINLESS-STEELS ; INDUCED PLASTICITY STEEL ; X80 PIPELINE STEEL ; HIGH-STRENGTH ; TENSILE PROPERTIES ; FCC CRYSTALS ; IN-SITU ; METALS ; STRAIN ; SUSCEPTIBILITY
WOS研究方向Nanoscience & Nanotechnology ; Materials Science, Multidisciplinary ; Metallurgy & Metallurgical Engineering
语种英语
WOS记录号WOS:000447573400017
资助机构National Key Research and Development Program of China [2017YFB0702003] ; NSFC [11472287, 11790292, 11572324] ; Strategic Priority Research Program of the Chinese Academy of Sciences [XDB22040302, XDB22040303] ; Key Research Program of Frontier Sciences [QYZDJSSW-JSC011]
源URL[http://dspace.imech.ac.cn/handle/311007/78144]  
专题力学研究所_非线性力学国家重点实验室
作者单位1.[Pu, Z.
2.Chen, Y.
3.Dai, L. H.] Chinese Acad Sci, Inst Mech, State Key Lab Nonlinear Mech, Beijing 100190, Peoples R China
4.Dai, L. H.] Univ Chinese Acad Sci, Sch Engn Sci, Beijing 101408, Peoples R China
5.[Dai, L. H.] Beijing Inst Technol, State Key Lab Explos Sci & Technol, Beijing 100081, Peoples R China
推荐引用方式
GB/T 7714
Pu Z,Chen Y,Dai LH. Strong resistance to hydrogen embrittlement of high-entropy alloy[J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING,2018,736:156-166.
APA Pu Z,Chen Y,&Dai LH.(2018).Strong resistance to hydrogen embrittlement of high-entropy alloy.MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING,736,156-166.
MLA Pu Z,et al."Strong resistance to hydrogen embrittlement of high-entropy alloy".MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING 736(2018):156-166.

入库方式: OAI收割

来源:力学研究所

浏览0
下载0
收藏0
其他版本

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。