Electrode catalysts behavior during direct ethanol fuel cell life-time test
文献类型:期刊论文
作者 | Jiang, LH; Sun, GQ; Wang, SL; Wang, GX; Xin, Q; Zhou, ZH; Zhou, B |
刊名 | electrochemistry communications
![]() |
出版日期 | 2005-07-01 |
卷号 | 7期号:7页码:663-668 |
关键词 | direct ethanol fuel cell electrocatalyst carbon supported platinum PtSn life time |
产权排序 | 1;1 |
通讯作者 | 辛勤 |
英文摘要 | in the present paper, a 60 h life-time test of a direct ethanol fuel cell (defc) at a current density of 20 ma cm(-2) (the beginning 38 h) and 40 ma cm(-2) (the last 22 h) was carried out. after the life-time test, the mea could not achieve the former performance. x-ray diffraction (xrd), transmission electron microscopy (tem) and energy dispersive x-ray analysis (edx) were employed to characterize the anode and cathode catalyst before and after the life-time test. the xrd and tem results showed that the particle size of the anode catalyst increased from 2.3 to 3.3 nm and the cathode from 3.0 to 4.6 nm. the edx results of ptsn/c anode catalysts before and after the life-time test indicated that the content of the oxygen and tin, especially the content of the platinum, decreased prominently after the life-time test. the results suggest that the agglomeration of electrocatalysts, the destruction of the anode catalyst together with the fuel/water crossover from anode to cathode concurrently contribute to the performance degradation of the defc. (c) 2005 elsevier b.v. all rights reserved. |
WOS标题词 | science & technology ; physical sciences |
类目[WOS] | electrochemistry |
研究领域[WOS] | electrochemistry |
关键词[WOS] | anode catalysts ; performance ; degradation ; dmfc |
收录类别 | SCI |
原文出处 | true |
语种 | 英语 |
WOS记录号 | WOS:000230251400005 |
公开日期 | 2010-11-30 |
源URL | [http://159.226.238.44/handle/321008/92751] ![]() |
专题 | 大连化学物理研究所_中国科学院大连化学物理研究所 |
作者单位 | 1.Chinese Acad Sci, Dalian Inst Chem Phys, Direct Methanol Fuel Cell Lab, Dalian 116023, Peoples R China 2.Chinese Acad Sci, Grad Sch, Beijing 100039, Peoples R China 3.Chinese Acad Sci, Dalian Inst Chem Phys, State Key Lab Catalysis, Dalian 116023, Peoples R China 4.Headwaters Nanokinetix, Lawrenceville, NJ 08648 USA |
推荐引用方式 GB/T 7714 | Jiang, LH,Sun, GQ,Wang, SL,et al. Electrode catalysts behavior during direct ethanol fuel cell life-time test[J]. electrochemistry communications,2005,7(7):663-668. |
APA | Jiang, LH.,Sun, GQ.,Wang, SL.,Wang, GX.,Xin, Q.,...&Zhou, B.(2005).Electrode catalysts behavior during direct ethanol fuel cell life-time test.electrochemistry communications,7(7),663-668. |
MLA | Jiang, LH,et al."Electrode catalysts behavior during direct ethanol fuel cell life-time test".electrochemistry communications 7.7(2005):663-668. |
入库方式: OAI收割
来源:大连化学物理研究所
浏览0
下载0
收藏0
其他版本
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。