Investigation on reactivity of iron nickel oxides in chemical looping dry reforming

文献类型:期刊论文

作者Huang, Zhen1,2,3; He, Fang1,2; Chen, Dezhen3; Zhao, Kun1,2; Wei, Guoqiang1,2; Zheng, Anqing1,2; Zhao, Zengli1,2; Li, Haibin1,2
刊名ENERGY
出版日期2016-12-01
卷号116页码:53-63
关键词Chemical Looping Dry Reforming (Cldr) Iron Nickel Oxides Synergistic Effect Spinel Structure Co2 Utilization
ISSN号0360-5442
DOI10.1016/j.energy.2016.09.101
文献子类Article
英文摘要Iron nickel oxides as oxygen carriers were investigated to clarify the reaction mechanism of NiFe2O4 material during the chemical looping dry reforming (CLDR) process. The thermodynamic analysis showed that metallic Fe can be oxidized into Fe3O4 by CO2, but metallic Ni carinot. The oxidizability of the four oxygen carriers was in the order of NiO > synthetic NiFe2O4 spinet > NiO-Fe2O3 mixed oxides > Fe2O3, and the reducibility sequence of their reduced products was synthetic NiFe2O4 spinel > NiO-Fe2O3 mixed oxides > Fe2O3 > NiO. The NiO showed the best oxidizability but it was easy to cause CH4 cracking and its reduced product (Ni) did not recover lattice oxygen under CO2 atmosphere. It only produced 74 mL CO for 1 g Fe2O3 during the CO2 reforming because of its weak oxidizability. The Redox ability of synthetic NiFe2O4 was obvious higher than that of NiO-Fe2O3 mixed oxides due to the synergistic effect of metallic Fe-Ni in the spinel structure. I g synthetic NiFe2O4 can produce 238 mL CO, which was twice higher than that of 1 g NiO-Fe2O3 mixed oxides (111 mL). A part of Fe element was divorced from the NiFe2O4 spinel structure after one cycle, which was the major reason for degradation of reactivity of NiFe2O4 oxygen carrier. (C) 2016 Elsevier Ltd. All rights reserved.
WOS关键词OXYGEN UNCOUPLING CLOU ; FLUIDIZED-BED REACTOR ; MN-FE OXIDES ; CO2 DECOMPOSITION ; POWER-PLANT ; MAGNETIC-PROPERTIES ; COMBUSTION ; CARRIER ; METHANE ; CARBON
语种英语
WOS记录号WOS:000389089000006
出版者PERGAMON-ELSEVIER SCIENCE LTD
资助机构National Natural Science Foundation of China(51406214 ; Natural Science Foundation of Guangdong Province(2015A030313719) ; Science & Technology Research Project of Guangdong Province(2013B050800008 ; 51406208) ; 2015A010106009)
源URL[http://ir.giec.ac.cn/handle/344007/13981]  
专题中国科学院广州能源研究所
通讯作者He, Fang; Chen, Dezhen
作者单位1.Chinese Acad Sci, Guangzhou Inst Energy Convers, Key Lab Renewable Energy, Beijing, Peoples R China
2.Chinese Acad Sci, Guangzhou Inst Energy Convers, Guangdong Key Lab New & Renewable Energy Res & De, Beijing, Peoples R China
3.Tongji Univ, Thermal & Environm Engn Inst, Shanghai, Peoples R China
推荐引用方式
GB/T 7714
Huang, Zhen,He, Fang,Chen, Dezhen,et al. Investigation on reactivity of iron nickel oxides in chemical looping dry reforming[J]. ENERGY,2016,116:53-63.
APA Huang, Zhen.,He, Fang.,Chen, Dezhen.,Zhao, Kun.,Wei, Guoqiang.,...&Li, Haibin.(2016).Investigation on reactivity of iron nickel oxides in chemical looping dry reforming.ENERGY,116,53-63.
MLA Huang, Zhen,et al."Investigation on reactivity of iron nickel oxides in chemical looping dry reforming".ENERGY 116(2016):53-63.

入库方式: OAI收割

来源:广州能源研究所

浏览0
下载0
收藏0
其他版本

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。