Organosoluble semi-alicyclic polyimides derived from 3,4-dicarboxy-1,2,3,4-tetrahydro-6-tert-buty1-1-naphthalene succinic dianhydride and aromatic diamines: Synthesis, characterization and thermal degradation investigation
文献类型:期刊论文
作者 | Guo, Yuan-zheng; Shen, Deng-xiong; Ni, Hong-jiang; Liu, Jin-gang; Yang, Shi-yong |
刊名 | PROGRESS IN ORGANIC COATINGS
![]() |
出版日期 | 2013-04-01 |
卷号 | 76期号:4页码:768-777 |
关键词 | Polyimide Alicyclic Dianhydride Solubility Transparency Thermal Degradation |
ISSN号 | 0300-9440 |
DOI | 10.1016/j.porgcoat.2013.01.006 |
英文摘要 | Semi-acyclic polyimides (PI-1-PI-4) have been prepared from a newly-developed alicyclic dianhydride, 3,4-dicarboxy-1,2,3,4-tetrahydro-6-tert-buty1-1-naphthalene succinic dianhydride (TTDA) and various aromatic diamines. The asymmetrical alicyclic tetralin structure in TTDA endowed the derived PI resins good solubility in various organic solvents. They were soluble not only in polar aprotic solvents but also in solvents with low boiling points including dichloromethane and tetrahydrofuran. Flexible and tough PI films were successfully cast from their N-methyl-2-pyrrolidone (NMP) solution except PI-1 derived from TTDA and 4,4'-oxydianiline (ODA). The PI films exhibited good optical transparency in the ultraviolet and visible light region with optical transmittances around 80% at a wavelength of 400 nm. The PI films showed good thermal stability up to 400 degrees C in nitrogen, after that they thermally decomposed rapidly. The thermal degradation behaviors of the Pls were investigated by means of thermogravimetric analysis-mass spectrometry (TG-MS), thermogravimetric analysis-Fourier transform infrared spectrometry (TG-FTIR) and the real time FTIR spectra (RT-FTIR) analysis techniques. The results revealed that the decomposition of PI-1 (as a representative) took place mainly in the range of 450-550 degrees C. The major degradative fragments at 500 degrees C were clearly identified as the tert-butyl-substituted tetralin moiety and its dealkylation products. Therefore, it can be deduced that for the TTDA-Pls, the single bond bridge attached the maleic anhydride and tetralin anhydride units in TTDA moiety might break first during the heating; thus producing the tetralin fragments. Crown Copyright (C) 2013 Published by Elsevier B.V. All rights reserved. |
语种 | 英语 |
WOS记录号 | WOS:000316425000033 |
出版者 | ELSEVIER SCIENCE SA |
源URL | [http://ir.iccas.ac.cn/handle/121111/53809] ![]() |
专题 | 中国科学院化学研究所 |
通讯作者 | Liu, Jin-gang |
作者单位 | Chinese Acad Sci, Inst Chem, Lab Adv Polymer Mat, Beijing 100190, Peoples R China |
推荐引用方式 GB/T 7714 | Guo, Yuan-zheng,Shen, Deng-xiong,Ni, Hong-jiang,et al. Organosoluble semi-alicyclic polyimides derived from 3,4-dicarboxy-1,2,3,4-tetrahydro-6-tert-buty1-1-naphthalene succinic dianhydride and aromatic diamines: Synthesis, characterization and thermal degradation investigation[J]. PROGRESS IN ORGANIC COATINGS,2013,76(4):768-777. |
APA | Guo, Yuan-zheng,Shen, Deng-xiong,Ni, Hong-jiang,Liu, Jin-gang,&Yang, Shi-yong.(2013).Organosoluble semi-alicyclic polyimides derived from 3,4-dicarboxy-1,2,3,4-tetrahydro-6-tert-buty1-1-naphthalene succinic dianhydride and aromatic diamines: Synthesis, characterization and thermal degradation investigation.PROGRESS IN ORGANIC COATINGS,76(4),768-777. |
MLA | Guo, Yuan-zheng,et al."Organosoluble semi-alicyclic polyimides derived from 3,4-dicarboxy-1,2,3,4-tetrahydro-6-tert-buty1-1-naphthalene succinic dianhydride and aromatic diamines: Synthesis, characterization and thermal degradation investigation".PROGRESS IN ORGANIC COATINGS 76.4(2013):768-777. |
入库方式: OAI收割
来源:化学研究所
浏览0
下载0
收藏0
其他版本
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。