关键词玻璃体 重金属 等离子体 氧硅比
其他题名Formation mechanism of vitrified slag and heavy metal fixed efficiency
通讯作者张金龙
产权排序中国科学院力学研究所;
中文摘要引入氧硅比的概念,阐述等离子体熔融玻璃化技术中玻璃体的形成机理,并且用实验加以验证。使用30kW直流等离子体电弧炉研究影响重金属固定效率的主要因素,按照正交实验表L16(44×23)安排实验,考察氧硅比、碱基度、重金属浓度、处理温度、处理时间、飞灰种类和物料形态共7种因素的影响作用。实验结果表明:对重金属As、Pb、Zn,处理温度和重金属浓度的影响作用最为显著,随着温度升高固定效率下降,随着重金属浓度的升高,固定效率先升高再降低,并在重金属浓度6000mg.kg-1时出现极大值;对重金属Cr,7种因素影响作用都很小。把玻璃化过程分为4个阶段,其中初期的挥发段是重金属的主要挥发阶段。
英文摘要Plasma technology is international advanced technology to destroy various types of hazardous wastes.The vitrified slag can form in the process of plasma treatment of inorganic wastes and effectively fix heavy metals,and its leaching rate is very low.Explained the formation mechanism of vitrified slag using the concept of silicon-oxygen ratio,and verified by experiment.Concluded that the vitrified slag can form at silicon-oxygen ratio less than 3,and crystal will grow at silicon-oxygen ratio more than 3.Find out the most important factors among 7 factors,including silicon-oxygen ratio,basicity,heavy metal contents,temperature,treating time,fly-ash types and constituents,to the heavy metal fixed efficiency using a 30 kW DC plasma arc reactor system.Concluded that the temperature and the heavy metal contents are the most important factors and directly influenced the heavy metal As,Pb and Zn fixed efficiency,the other 5 factors little effect on the heavy metal fixed efficiency.With increasing temperature,the heavy metal fixed efficiency dropped.As the heavy metal contents increases,the heavy metal fixed efficiency increased and then decreased before,and reached a maximum value at 6mg·g-1.But all of 7 factors didn’t effect to the metal Cr fixed efficiency,the heavy metal Cr fixed efficiency are more than 85% in all experiments.The heavy metal fixed process is divided into 4 stages depend on the temperature of crucibles wall heated.80% of escape heavy metal run away at volatilization period which last 6—10 minutes from heat beginning.So how to control the heavy metals running away at volatilization period is the best way to improve the heavy metals fixed efficiency.
学科主题力学
资助信息中国科学院知识创新工程领域前沿项目
收录类别EI
原文出处http://epub3.cnki.net/grid2008/brief/detailj.aspx?filename=HGSZ2011S1039&dbname=CJFQ2011
语种中文
公开日期2012-03-31
源URL[http://dspace.imech.ac.cn/handle/311007/44870]  
专题力学研究所_等离子体与燃烧中心(2009-2011)
推荐引用方式
GB/T 7714
张金龙,李要建,王贵全,等. 玻璃体形成机理与重金属固定效率[J]. 化工学报,2011,62(S1):215-218.
APA 张金龙,李要建,王贵全,徐永香,&盛宏至.(2011).玻璃体形成机理与重金属固定效率.化工学报,62(S1),215-218.
MLA 张金龙,et al."玻璃体形成机理与重金属固定效率".化工学报 62.S1(2011):215-218.

入库方式: OAI收割

来源:力学研究所

浏览0
下载0
收藏0
其他版本

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。