中国科学院机构知识库网格
Chinese Academy of Sciences Institutional Repositories Grid
Surface strengthening of Ti(3)SiC(2) through magnetron sputtering of Mo and Zr and subsequent annealing

文献类型:期刊论文

作者H. P. Guo ; A. J. Li ; J. Zhang ; L. F. He ; Y. C. Zhou
刊名Journal of the European Ceramic Society
出版日期2010
卷号30期号:10页码:2123-2130
关键词Ti(3)SiC(2) Surface strengthening Magnetron sputtering Microhardness titanium-silicon carbide mechanical-properties oxidation behavior damage tolerance bulk ceramics microstructure temperature diffusion composites kinetics
ISSN号0955-2219
中文摘要Magnetron sputtering deposition of Mo and Zr and subsequent annealing were conducted with the motivation to modify the surface hardness of Ti(3)SiC(2). For Mo-coated Ti(3)SiC(2), Si diffused outward into the Mo layer and reacted with Mo to form molybdenum silicides in the temperature range of 1000-1100 degrees C. The MoSi(2) layer, however, cracked and easily spalled off. For Zr-coated Ti(3)SiC(2), Si also diffused outward to form Zr-Si intermetallic compounds at 900-1100 degrees C. The Zr-Si compounds layer had good adhesion with Ti(3)SiC(2) substrate, which resulted in the increased surface hardness. (c) 2010 Elsevier Ltd. All rights reserved.
原文出处://WOS:000278651400017
公开日期2012-04-13
源URL[http://210.72.142.130/handle/321006/31126]  
专题金属研究所_中国科学院金属研究所
推荐引用方式
GB/T 7714
H. P. Guo,A. J. Li,J. Zhang,et al. Surface strengthening of Ti(3)SiC(2) through magnetron sputtering of Mo and Zr and subsequent annealing[J]. Journal of the European Ceramic Society,2010,30(10):2123-2130.
APA H. P. Guo,A. J. Li,J. Zhang,L. F. He,&Y. C. Zhou.(2010).Surface strengthening of Ti(3)SiC(2) through magnetron sputtering of Mo and Zr and subsequent annealing.Journal of the European Ceramic Society,30(10),2123-2130.
MLA H. P. Guo,et al."Surface strengthening of Ti(3)SiC(2) through magnetron sputtering of Mo and Zr and subsequent annealing".Journal of the European Ceramic Society 30.10(2010):2123-2130.