Corrosion behavior of AZ31 magnesium alloy in simulated acid rain solution

文献类型:期刊论文

作者F. Liu ; Y. W. Song ; D. Y. Shan ; E. H. Han
刊名Transactions of Nonferrous Metals Society of China
出版日期2010
卷号20页码:S638-S642
关键词AZ31 magnesium alloy simulated acid rain solution Cl(-) ion AlMn phase in-situ observation wet-dry conditions sodium-chloride az91
ISSN号1003-6326
中文摘要The corrosion mechanism of AZ31 magnesium alloy used as automobile components and the influence of the concentration of Cl(-) ion in simulated acid rain (SAR) were studied by electrochemical tests and SEM. The results show that pitting corrosion happens around the AlMn phases locating at the grain boundary. The corrosion of AZ31 magnesium alloy in SAR is controlled by the rate of anodic dissolution and hydrogen evolution, and the corrosion rate of AZ31 increases with increasing concentration of Cl(-) ion. However, the Cl(-) ion in SAR is not the main influencing factor inducing the pitting corrosion.
原文出处://WOS:000280873300067
公开日期2012-04-13
源URL[http://210.72.142.130/handle/321006/31275]  
专题金属研究所_中国科学院金属研究所
推荐引用方式
GB/T 7714
F. Liu,Y. W. Song,D. Y. Shan,et al. Corrosion behavior of AZ31 magnesium alloy in simulated acid rain solution[J]. Transactions of Nonferrous Metals Society of China,2010,20:S638-S642.
APA F. Liu,Y. W. Song,D. Y. Shan,&E. H. Han.(2010).Corrosion behavior of AZ31 magnesium alloy in simulated acid rain solution.Transactions of Nonferrous Metals Society of China,20,S638-S642.