Pit growth in a Ni-Nb metallic glass compared with its crystalline counterpart

文献类型:期刊论文

作者Z. M. Wang ; J. Zhang ; J. Q. Wang
刊名Intermetallics
出版日期2010
卷号18期号:11页码:2077-2082
关键词Corrosion Glasses metallic Corrosion behaviour Electrochemical characterization high corrosion-resistance amorphous-metal mechanical-properties pitting corrosion crevice corrosion alloys behavior cr mo initiation
ISSN号0966-9795
中文摘要The growth and repassivation behavior of metastable pits in a Ni(50)Nb(50) metallic glass, as well as its crystalline counterpart, were investigated by statistical analysis on the current transients in potentio-static measurements The results show that amorphous Ni(50)Nb(50) sample demonstrates a higher transient current, shorter pit growth and repassivation times than the crystallized sample Comparisons of pit growth rates and charges passed during pitting reveal that pits in amorphous alloy grow faster but with smaller final pit volumes. Iris suggested that amorphous structure can induce rapid dissolution in pits and thus promote the accumulation of passivating elements (Nb), resulting in a higher repassivation rate A notable effect of amorphous structure on the early growth of pits is determined. (C) 2010 Elsevier Ltd All rights reserved
原文出处://WOS:000282710400010
公开日期2012-04-13
源URL[http://210.72.142.130/handle/321006/31564]  
专题金属研究所_中国科学院金属研究所
推荐引用方式
GB/T 7714
Z. M. Wang,J. Zhang,J. Q. Wang. Pit growth in a Ni-Nb metallic glass compared with its crystalline counterpart[J]. Intermetallics,2010,18(11):2077-2082.
APA Z. M. Wang,J. Zhang,&J. Q. Wang.(2010).Pit growth in a Ni-Nb metallic glass compared with its crystalline counterpart.Intermetallics,18(11),2077-2082.
MLA Z. M. Wang,et al."Pit growth in a Ni-Nb metallic glass compared with its crystalline counterpart".Intermetallics 18.11(2010):2077-2082.

入库方式: OAI收割

来源:金属研究所

浏览0
下载0
收藏0
其他版本

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。