Abnormal Oxidation Kinetics of Fe-Cr-Al Alloys at 1273 K Induced by Cr-rich Phases
文献类型:期刊论文
作者 | Z. G. Zhang ; Y. L. Mao ; Y. Xie ; C. M. Hou ; Z. J. Feng |
刊名 | High Temperature Materials and Processes
![]() |
出版日期 | 2010 |
卷号 | 29期号:1-2页码:27-33 |
关键词 | Fe-Cr-Al alloy Cr-rich phase High temperature oxidation high-temperature oxidation chromium-aluminum alloys protective scales forming alloys behavior growth ods microstructure fe-20cr-5al yttrium |
ISSN号 | 0334-6455 |
中文摘要 | The oxidations of Fe-10Cr-10Al, Fe-15Cr-10Al, and Fe-20Cr-10Al (all in at.%) alloys were conducted in 0.1 MPa oxygen at 1273 K. After a transient oxidation stage, three alloys underwent a selective oxidation of Al incorporated with oxidation of Cr and then a steady state stage involving exclusive oxidation of Al. Compared with Fe-10Cr-10Al and Fe-20Cr-10Al, Fe-15Cr-10Al exhibited abnormal oxidation kinetics, i.e. the much higher oxidation rate during the selective oxidation of Al and the much lower oxidation rate during the exclusive oxidation of Al. The abnormal oxidation kinetics of Fe-15Cr-10Al was induced by the Cr-rich phases existing parallel to the surface of the specimens. |
原文出处 | |
公开日期 | 2012-04-13 |
源URL | [http://ir.imr.ac.cn/handle/321006/31735] ![]() |
专题 | 金属研究所_中国科学院金属研究所 |
推荐引用方式 GB/T 7714 | Z. G. Zhang,Y. L. Mao,Y. Xie,et al. Abnormal Oxidation Kinetics of Fe-Cr-Al Alloys at 1273 K Induced by Cr-rich Phases[J]. High Temperature Materials and Processes,2010,29(1-2):27-33. |
APA | Z. G. Zhang,Y. L. Mao,Y. Xie,C. M. Hou,&Z. J. Feng.(2010).Abnormal Oxidation Kinetics of Fe-Cr-Al Alloys at 1273 K Induced by Cr-rich Phases.High Temperature Materials and Processes,29(1-2),27-33. |
MLA | Z. G. Zhang,et al."Abnormal Oxidation Kinetics of Fe-Cr-Al Alloys at 1273 K Induced by Cr-rich Phases".High Temperature Materials and Processes 29.1-2(2010):27-33. |
入库方式: OAI收割
来源:金属研究所
浏览0
下载0
收藏0
其他版本
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。