中文摘要The early stages of the evolution of atmospheric corrosion of carbon steels exposed in both a laboratory simulated and a natural atmosphere environment in Shenyang have been observed by in situ scanning electron microscopy. In the case of laboratory cyclic wet-dry tests, even though the chloride content level is very low, filiform corrosion is initiated in the early stage. The filiform corrosion grows in random directions, forming a network of ridges. White nodules nucleate and grow on the ridges during continued corrosion and eventually connect with each other to form the initial corrosion scale. Pits were also found on the surface beneath corrosion products. In the case of a natural atmospheric environment, both filiform corrosion and other localized corrosion, such as pitting and inter-granular attack take place in the initial stage. It is obvious that there is variety of localized corrosion in the initial stage of atmospheric corrosion. (C) 2007 Elsevier Ltd. All rights reserved.
原文出处://WOS:000248039500009
公开日期2012-04-13
源URL[http://ir.imr.ac.cn/handle/321006/33563]  
专题金属研究所_中国科学院金属研究所
推荐引用方式
GB/T 7714
W. Han,G. C. Yu,Z. Y. Wang,et al. Characterisation of initial atmospheric corrosion carbon steels by field exposure and laboratory simulation[J]. Corrosion Science,2007,49(7):2920-2935.
APA W. Han,G. C. Yu,Z. Y. Wang,&J. Wang.(2007).Characterisation of initial atmospheric corrosion carbon steels by field exposure and laboratory simulation.Corrosion Science,49(7),2920-2935.
MLA W. Han,et al."Characterisation of initial atmospheric corrosion carbon steels by field exposure and laboratory simulation".Corrosion Science 49.7(2007):2920-2935.

入库方式: OAI收割

来源:金属研究所

浏览0
下载0
收藏0
其他版本

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。