Initial deposition mechanism of electroless nickel plating on AZ91D magnesium alloys
文献类型:期刊论文
作者 | Y. Song ; D. Shan ; E. Han |
刊名 | Canadian Metallurgical Quarterly
![]() |
出版日期 | 2006 |
卷号 | 45期号:2页码:215-222 |
关键词 | corrosion pretreatment |
ISSN号 | 0008-4433 |
中文摘要 | The pretreatment processes and initial deposition mechanism of electroless nickel plating on AZ91D magnesium alloy were investigated by scanning electron microscopy (SEM) and energy dispersive X-ray (EDX). The results showed that alkaline cleaning could remove the greases and oils from the substrate surface. Acid etching could wipe off the metal chippings and oxides. The hydrofluoric acid activating process which could improve the adhesion of coating to substrate played a key role in the subsequent process of electroless nickel plating. The nickel coating was deposited preferentially on the primary alpha phase and then spread to the eutectic alpha phase and beta phase. The nickel initially nucleated on the primary alpha phase by a replacement reaction, then grew depending on the autocatalysis function of nickel. The coating on the beta phase displayed better adhesion than that on the alpha phase due to the nails fixing effect |
原文出处 | |
公开日期 | 2012-04-14 |
源URL | [http://ir.imr.ac.cn/handle/321006/34460] ![]() |
专题 | 金属研究所_中国科学院金属研究所 |
推荐引用方式 GB/T 7714 | Y. Song,D. Shan,E. Han. Initial deposition mechanism of electroless nickel plating on AZ91D magnesium alloys[J]. Canadian Metallurgical Quarterly,2006,45(2):215-222. |
APA | Y. Song,D. Shan,&E. Han.(2006).Initial deposition mechanism of electroless nickel plating on AZ91D magnesium alloys.Canadian Metallurgical Quarterly,45(2),215-222. |
MLA | Y. Song,et al."Initial deposition mechanism of electroless nickel plating on AZ91D magnesium alloys".Canadian Metallurgical Quarterly 45.2(2006):215-222. |
入库方式: OAI收割
来源:金属研究所
浏览0
下载0
收藏0
其他版本
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。