Oxidation of the single-crystal Ni-base superalloy DD32 containing rhenium in air at 900 and 1000 degrees C

文献类型:期刊论文

作者C. T. Liu ; X. F. Sun ; H. R. Guan ; Z. Q. Hu
刊名Surface & Coatings Technology
出版日期2005
卷号197期号:1页码:39-44
关键词single-crystal (SC) superalloy oxidation NiO alpha-Al2O3 stress rupture behavior cr-al alloys microstructure coatings
ISSN号0257-8972
中文摘要The oxidation behavior of a single-crystal Ni-base superalloy DD32 was studied in air at 900 and 1000 ° C. The oxide morphology and microstructure were analyzed by X-ray diffraction (XRD), SEM/EDS. The scales formed at 900 and 1000 ° C were complicated, with an outer layer of columnar NiO, an intermediate layer mainly composed of complex oxides and a small amount of spinels, and an inner continuous layer of α-Al2O3. At 900 and 1000 ° C, two oxidation steps appear in the oxidation kinetics. The first one is controlled by NiO growth and the second by Al2O3 growth once a continuous Al2O3 layer formed under the previously grown NiO layer after a critical time. © 2004 Elsevier BY. All rights reserved.
原文出处://WOS:000229513700005
公开日期2012-04-14
源URL[http://ir.imr.ac.cn/handle/321006/34929]  
专题金属研究所_中国科学院金属研究所
推荐引用方式
GB/T 7714
C. T. Liu,X. F. Sun,H. R. Guan,et al. Oxidation of the single-crystal Ni-base superalloy DD32 containing rhenium in air at 900 and 1000 degrees C[J]. Surface & Coatings Technology,2005,197(1):39-44.
APA C. T. Liu,X. F. Sun,H. R. Guan,&Z. Q. Hu.(2005).Oxidation of the single-crystal Ni-base superalloy DD32 containing rhenium in air at 900 and 1000 degrees C.Surface & Coatings Technology,197(1),39-44.
MLA C. T. Liu,et al."Oxidation of the single-crystal Ni-base superalloy DD32 containing rhenium in air at 900 and 1000 degrees C".Surface & Coatings Technology 197.1(2005):39-44.

入库方式: OAI收割

来源:金属研究所

浏览0
下载0
收藏0
其他版本

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。