掺Co(2+)的富铝Mg(0.4)Al(2.4)O(4)尖晶石作为饱和吸收体的二极管泵浦铒玻璃1535微芯激光
文献类型:期刊论文
作者 | 姜大朋 ; 邹宇琦 ; 苏良碧 ; 唐慧丽 ; 99 ; 郑丽和 ; 李红军 ; 徐军 |
刊名 | Laser Phys. Lett.
![]() |
出版日期 | 2011-12-07 |
ISSN号 | 1612-2011 |
其他题名 | A Co(2+)-doped alumina-rich Mg(0.4)Al(2.4)O(4) spinel crystal as saturable absorber for a LD pumped Er: glass microchip laser at 1535 nm |
通讯作者 | Y.Q. Zou |
中文摘要 | Co2+-doped Mg0.4Al2.4O4 single crystal up to ?28×40 mm3 was successfully grown by the Czochralski method. By using this crystal as saturable absorber, we have demonstrated a diode-end-pumped passively Q-switched Er:glass microchip laser operating at 1535 nm for the first time to the best of our knowledge. The dependences of average output power, repetition rate and pulse energy on the incident pump power were investigated. In the passive Q-switching regime, a maximum average output power of 22.12 mW was btained at the incident pump power of 410 mW. The narrowest pulse width, the largest pulse energy and the highest peak power were obtained to be about 3.5 ns, 4.8 μJ, and 1.37 kW, respectively. |
学科主题 | 人工晶体 |
收录类别 | SCI收录 |
语种 | 英语 |
公开日期 | 2012-07-03 |
源URL | [http://ir.sic.ac.cn/handle/331005/850] ![]() |
专题 | 上海硅酸盐研究所_人工晶体研究中心_期刊论文 |
推荐引用方式 GB/T 7714 | 姜大朋,邹宇琦,苏良碧,等. 掺Co(2+)的富铝Mg(0.4)Al(2.4)O(4)尖晶石作为饱和吸收体的二极管泵浦铒玻璃1535微芯激光[J]. Laser Phys. Lett.,2011. |
APA | 姜大朋.,邹宇琦.,苏良碧.,唐慧丽.,99.,...&徐军.(2011).掺Co(2+)的富铝Mg(0.4)Al(2.4)O(4)尖晶石作为饱和吸收体的二极管泵浦铒玻璃1535微芯激光.Laser Phys. Lett.. |
MLA | 姜大朋,et al."掺Co(2+)的富铝Mg(0.4)Al(2.4)O(4)尖晶石作为饱和吸收体的二极管泵浦铒玻璃1535微芯激光".Laser Phys. Lett. (2011). |
入库方式: OAI收割
来源:上海硅酸盐研究所
浏览0
下载0
收藏0
其他版本
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。