Dynamic fracture behavious of Fe-Mo-Si-B amorphous alloy ribbon
文献类型:期刊论文
作者 | Gan, Y |
刊名 | ACTA METALLURGICA SINICA
![]() |
出版日期 | 2001-06-18 |
卷号 | 37期号:6页码:585-588 |
关键词 | amorphous alloy dynamic fracture crack branching stress wave induced cracking (SWIC) |
ISSN号 | 0412-1961 |
通讯作者 | Gan, Y() |
英文摘要 | Dynamic fracture characteristics have been observed and interpreted for Fe-Mo-Si-B amorphous alloy ribbon. Crack branching and stress wave induced cracking are the main features of dynamic fracture. Branching of main crack occurs when the crack tip intensity factor reaches the critical value K-IB = 35 MPa(.)m(1/2), and the corresponding plane strain fracture toughness K-Ic = 16 MPa(.)m(1/2). It is deduced that crack branching is the necessary condition for generation of compressive longitudinal wave. Stress wave induced cracking occurs when the amplitude of reflected compressive longitudinal wave reaches the tensile strength. |
WOS研究方向 | Metallurgy & Metallurgical Engineering |
语种 | 英语 |
WOS记录号 | WOS:000172766900006 |
出版者 | SCIENCE CHINA PRESS |
源URL | [http://ir.imr.ac.cn/handle/321006/112293] ![]() |
专题 | 金属研究所_中国科学院金属研究所 |
通讯作者 | Gan, Y |
作者单位 | Chinese Acad Sci, Met Res Inst, Shenyang 110016, Peoples R China |
推荐引用方式 GB/T 7714 | Gan, Y. Dynamic fracture behavious of Fe-Mo-Si-B amorphous alloy ribbon[J]. ACTA METALLURGICA SINICA,2001,37(6):585-588. |
APA | Gan, Y.(2001).Dynamic fracture behavious of Fe-Mo-Si-B amorphous alloy ribbon.ACTA METALLURGICA SINICA,37(6),585-588. |
MLA | Gan, Y."Dynamic fracture behavious of Fe-Mo-Si-B amorphous alloy ribbon".ACTA METALLURGICA SINICA 37.6(2001):585-588. |