Corrosion and Cavitation Erosion Behaviours of Cast Nickel Aluminium Bronze in 3.5% NaCl Solution with Different Sulphide Concentrations

文献类型:期刊论文

作者Song, Qi-Ning2; Xu, Nan2; Tong, Yao2; Huang, Chen-Ming2; Sun, Shou-Yu2; Xu, Chen-Bo2; Bao, Ye-Feng2; Jiang, Yong-Feng2; Qiao, Yan-Xin1; Zhu, Zhi-Yuan1
刊名ACTA METALLURGICA SINICA-ENGLISH LETTERS
出版日期2019-12-01
卷号32期号:12页码:1470-1482
ISSN号1006-7191
关键词Nickel aluminium bronze Sulphide Corrosion Cavitation erosion Synergy
DOI10.1007/s40195-019-00963-7
通讯作者Song, Qi-Ning(qnsong@hhu.edu.cn)
英文摘要The effect of sulphide (Na2S) concentration (SC) on the corrosion and cavitation erosion behaviours of a cast nickel aluminium bronze (NAB) in 3.5% NaCl solution is investigated in this study. The results show that when the SC exceeds 50 ppm, the hydrogen evolution reaction dominates the cathodic process, and a limiting current region appears in the anodic branch of the polarisation curve due to the formation of a copper sulphide film, which is a diffusion-controlled process. After long-term immersion, the increased mass loss rate of NAB with the sulphide additions of 20 and 50 ppm is attributed to the less protective films, which contains a mixture of copper oxides and sulphides. Moreover, NAB undergoes severe localised corrosion (selective phase corrosion, SPC) at the beta ' phases and eutectoid microstructure alpha + kappa(III). By comparison, NAB undergoes general corrosion and a copper sulphide film is formed in 100 and 200 ppm sulphide solutions. Cavitation erosion greatly increases the corrosion rate of NAB in all solutions and causes a negative potential shift in 3.5% NaCl solution due to the film destruction. However, a positive potential shift occurs in the solutions with SC higher than 50 ppm due to the accelerated mass transfer of the cathodic process. The cavitation erosion mass loss rate of NAB increases with the increase of SC. The occurrence of severe SPC decreases the phase boundary cohesion and causes brittle fracture under the cavitation impact. The corrosion-enhanced erosion is the most predominant factor for the cavitation erosion damage when the SC exceeds 50 ppm.
资助项目National Natural Science Foundation of China[51601058] ; National Natural Science Foundation of China[51879089] ; Fundamental Research Funds for the Central Universities of P.R. China[2018B59614] ; Natural Science Foundation of Jiangsu Province[BK20191161] ; Changzhou Sci Tech Program[CJ20180045] ; first group of 2011 plan of China's Jiangsu province (Cooperative Innovational Center for Coastal Development Protection)[[2013] 56]
WOS研究方向Metallurgy & Metallurgical Engineering
语种英语
出版者CHINESE ACAD SCIENCES, INST METAL RESEARCH
WOS记录号WOS:000493679100002
资助机构National Natural Science Foundation of China ; Fundamental Research Funds for the Central Universities of P.R. China ; Natural Science Foundation of Jiangsu Province ; Changzhou Sci Tech Program ; first group of 2011 plan of China's Jiangsu province (Cooperative Innovational Center for Coastal Development Protection)
源URL[http://ir.imr.ac.cn/handle/321006/136960]  
专题金属研究所_中国科学院金属研究所
通讯作者Song, Qi-Ning
作者单位1.Jiangsu Univ Sci & Technol, Coll Mat Sci & Engn, 2 Mengxi Rd, Zhenjiang 212003, Jiangsu, Peoples R China
2.Hohai Univ, Coll Mech & Elect Engn, 200 Jinling North Rd, Changzhou 213022, Peoples R China
3.Chinese Acad Sci, Inst Met Res, Key Lab Nucl Mat & Safety Assessment, 62 Wencui Rd, Shenyang 110016, Liaoning, Peoples R China
推荐引用方式
GB/T 7714
Song, Qi-Ning,Xu, Nan,Tong, Yao,et al. Corrosion and Cavitation Erosion Behaviours of Cast Nickel Aluminium Bronze in 3.5% NaCl Solution with Different Sulphide Concentrations[J]. ACTA METALLURGICA SINICA-ENGLISH LETTERS,2019,32(12):1470-1482.
APA Song, Qi-Ning.,Xu, Nan.,Tong, Yao.,Huang, Chen-Ming.,Sun, Shou-Yu.,...&Wang, Zheng-Bin.(2019).Corrosion and Cavitation Erosion Behaviours of Cast Nickel Aluminium Bronze in 3.5% NaCl Solution with Different Sulphide Concentrations.ACTA METALLURGICA SINICA-ENGLISH LETTERS,32(12),1470-1482.
MLA Song, Qi-Ning,et al."Corrosion and Cavitation Erosion Behaviours of Cast Nickel Aluminium Bronze in 3.5% NaCl Solution with Different Sulphide Concentrations".ACTA METALLURGICA SINICA-ENGLISH LETTERS 32.12(2019):1470-1482.

入库方式: OAI收割

来源:金属研究所

浏览0
下载0
收藏0
其他版本

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。