Investigating the evolution of freckles into sliver defects in Ni-based single-crystal superalloy castings

文献类型:期刊论文

作者Han, Dongyu1,2; Jiang, Weiguo3; Xiao, Jiuhan1,2; Li, Kaiwen2,4; Lu, Yuzhang2; Lou, Langhong2
刊名MATERIALS TODAY COMMUNICATIONS
出版日期2021-06-01
卷号27页码:14
关键词Ni-based superalloys Directional solidification Freckle evolution Slivers
DOI10.1016/j.mtcomm.2021.102350
通讯作者Jiang, Weiguo(jwg@wfust.edu.cn)
英文摘要Freckles are detrimental solidification defects in Ni-based single-crystal superalloy castings that are formed during directional solidification. However, the evolution of freckles into sliver defects has rarely been reported, and the mechanism of this evolution is unclear. In this study, the evolution of freckles into slivers in the extended zone of casting was established to be the deformation of dendrites induced by the thermal contraction stress in the freckle channel. The morphology of the mushy zone was simulated using ProCAST, which indicated that freckles were formed at the highest position of the mushy zone. During the initiation of the slivers, deformation occurred at the freckle channel, indicating that the thermal contraction stress was a result of the solidification shrinkage of solute-rich liquid. The misorientation from the initial freckle grains to the slivers ranged from 15 degrees to 57 degrees. In addition, the orientation and ability of dendrite branching are crucial for the extension of the sliver dendrites.
资助项目National Natural Science Foundation of China[51674235] ; National Science and Technology Major Project of China[2017VI-0001-0070] ; National Key Research and Development Program of China[2017YFB0702904]
WOS研究方向Materials Science
语种英语
WOS记录号WOS:000683031100001
出版者ELSEVIER
资助机构National Natural Science Foundation of China ; National Science and Technology Major Project of China ; National Key Research and Development Program of China
源URL[http://ir.imr.ac.cn/handle/321006/159509]  
专题金属研究所_中国科学院金属研究所
通讯作者Jiang, Weiguo
作者单位1.Univ Sci & Technol China, Sch Mat Sci & Engn, Shenyang 110016, Peoples R China
2.Chinese Acad Sci, Inst Met Res, Shichangxu Innovat Ctr Adv Mat, Shenyang 110016, Peoples R China
3.Weifang Univ Sci & Technol, Shouguang 262700, Shandong, Peoples R China
4.Shenyang Univ Technol, Sch Mat Sci & Engn, Shenyang 110870, Peoples R China
推荐引用方式
GB/T 7714
Han, Dongyu,Jiang, Weiguo,Xiao, Jiuhan,et al. Investigating the evolution of freckles into sliver defects in Ni-based single-crystal superalloy castings[J]. MATERIALS TODAY COMMUNICATIONS,2021,27:14.
APA Han, Dongyu,Jiang, Weiguo,Xiao, Jiuhan,Li, Kaiwen,Lu, Yuzhang,&Lou, Langhong.(2021).Investigating the evolution of freckles into sliver defects in Ni-based single-crystal superalloy castings.MATERIALS TODAY COMMUNICATIONS,27,14.
MLA Han, Dongyu,et al."Investigating the evolution of freckles into sliver defects in Ni-based single-crystal superalloy castings".MATERIALS TODAY COMMUNICATIONS 27(2021):14.

入库方式: OAI收割

来源:金属研究所

浏览0
下载0
收藏0
其他版本

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。