Penetration Failure Mechanism of Multi-Diameter Tungsten Fiber Reinforced Zr-Based Bulk Metallic Glasses Matrix Composite Rod

文献类型:期刊论文

作者Du, Chengxin1,2; Fu, Huameng3; Zhu, Zhengwang3; Wang, Kehong1; Gao, Guangfa2; Zhou, Feng2; Xu, Lizhi2; Du, Zhonghua2
刊名CRYSTALS
出版日期2022-02-01
卷号12期号:2页码:16
关键词multi-diameter tungsten fiber-reinforced Zr-based bulk metallic glasses matrix composite tungsten fiber penetration failure mode bend space ultimate bending diameter
DOI10.3390/cryst12020124
通讯作者Gao, Guangfa(gfgao@ustc.edu.cn)
英文摘要In order to increase the penetration ability of tungsten fiber-reinforced Zr-based bulk metallic glasses matrix composite rod, two multi-diameter tungsten fiber-reinforced Zr-based bulk metallic glasses matrix composites (MD-WF/Zr-MG) are designed. In MD-WF/Zr-MG-I, the diameters of tungsten fiber (WF) increase gradually from the inside to outside, which is the opposite in MD-WF/Zr-MG-II. Penetration experiment of two kinds of MD-WF/Zr-MG rods into rolled homogeneous armor (RHA) steel target from 1470 m/s to 1630 m/s is conducted. The average penetration depth of the MD-WF/Zr-MG-II rod is higher than that of the MD-WF/Zr-MG-I rod. Penetration failure modes of MD-WF/Zr-MG-I and MD-WF/Zr-MG-II rods are bending, backflow of WFs and shear failure respectively. The failure mode of MD-WF/Zr-MG is affected by the bend spaces and the ultimate bending diameters of WFs. If the bend spaces of all WFs are equal or larger than their ultimate bending diameters, the penetration failure mode is the bending and backflow of WFs, oppositely the penetration failure mode is the shear failure. The MD-WF/Zr-MG rod with shear failure exhibits high penetration ability because of low penetration resistance and little residual material in the crater. When designing MD-WF/Zr-MG, bend spaces of a part of WFs should be smaller than their ultimate bending diameter to cause shear failure.
WOS研究方向Crystallography ; Materials Science
语种英语
WOS记录号WOS:000763424100001
出版者MDPI
源URL[http://ir.imr.ac.cn/handle/321006/173305]  
专题金属研究所_中国科学院金属研究所
通讯作者Gao, Guangfa
作者单位1.Nanjing Univ Sci & Technol, Sch Mat Sci & Engn, Nanjing 210094, Peoples R China
2.Nanjing Univ Sci & Technol, Sch Mech Engn, Nanjing 210094, Peoples R China
3.Chinese Acad Sci, Inst Met Res, Shenyang 110016, Peoples R China
推荐引用方式
GB/T 7714
Du, Chengxin,Fu, Huameng,Zhu, Zhengwang,et al. Penetration Failure Mechanism of Multi-Diameter Tungsten Fiber Reinforced Zr-Based Bulk Metallic Glasses Matrix Composite Rod[J]. CRYSTALS,2022,12(2):16.
APA Du, Chengxin.,Fu, Huameng.,Zhu, Zhengwang.,Wang, Kehong.,Gao, Guangfa.,...&Du, Zhonghua.(2022).Penetration Failure Mechanism of Multi-Diameter Tungsten Fiber Reinforced Zr-Based Bulk Metallic Glasses Matrix Composite Rod.CRYSTALS,12(2),16.
MLA Du, Chengxin,et al."Penetration Failure Mechanism of Multi-Diameter Tungsten Fiber Reinforced Zr-Based Bulk Metallic Glasses Matrix Composite Rod".CRYSTALS 12.2(2022):16.

入库方式: OAI收割

来源:金属研究所

浏览0
下载0
收藏0
其他版本

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。