Comparison of the Three-Phase Corrosion Behavior of SiN and 304L Stainless Steels in 6 M Nitric Acid Solution at Different Temperatures

文献类型:期刊论文

作者Sun, Shengxuan1,2; Zhang, Lianmin2; Ma, Aili2; Daniel, Enobong Felix2; Zhang, Chunzhi1; Zheng, Yugui2
刊名METALS
出版日期2022-06-01
卷号12期号:6页码:17
关键词stainless steel three-phase corrosion behavior nitric acid weight loss corrosion kinetics
DOI10.3390/met12060922
通讯作者Zhang, Lianmin(lmzhang14s@imr.ac.cn) ; Zhang, Chunzhi(czzhang@sdust.edu.cn)
英文摘要In this work, the three-phase corrosion behavior of SiN and 304L stainless steels was comparatively investigated in a 6 M nitric acid solution at different temperatures. It was found that the corrosion rates of both steels in the liquid phase, vapor phase and condensate phase of nitric acid showed an increasing trend with rising temperature. Meanwhile, there also existed some differences in the corrosion kinetics and the corrosion resistance in the different phases of nitric acid. The corrosion rate of SiN and 304L stainless steels in the liquid phase of nitric acid had a cubic function relationship with temperature, and SiN stainless steel presented better corrosion resistance without intergranular corrosion (IGC) compared with 304L stainless steel with IGC at 100 degrees C and 120 degrees C. By contrast, the SiN stainless steel displayed a lower corrosion resistance than 304L stainless steel in the vapor phase of nitric acid at the same temperature, and the corrosion rates of SiN and 304L stainless steels showed a quadratic function relationship with temperature, indicating a milder corrosion in the vapor phase in comparison with that in the liquid phase of nitric acid. In the condensate phase of nitric acid, there was a similar corrosion behavior of the two steels to that in the nitric acid vapor phase, and 304L stainless steel also demonstrated a better corrosion resistance than SiN stainless steel at the same temperature. The differences in corrosion behavior between the two steels could be attributed to the changed media environment and the different alloy composition, and the two aspects were discussed in detail based on relevant experimental results. This work can provide an important insight into the material selection for reprocessing equipment and the development of new corrosion-resistant materials used in spent fuel reprocessing.
资助项目China National Nuclear Corporation (CNNC) Science Fund for Talented Young Scholars ; National Natural Science Foundation of China[52101105] ; Chinese Postdoctoral Science Foundation[2020M670811]
WOS研究方向Materials Science ; Metallurgy & Metallurgical Engineering
语种英语
出版者MDPI
WOS记录号WOS:000819070600001
资助机构China National Nuclear Corporation (CNNC) Science Fund for Talented Young Scholars ; National Natural Science Foundation of China ; Chinese Postdoctoral Science Foundation
源URL[http://ir.imr.ac.cn/handle/321006/174951]  
专题金属研究所_中国科学院金属研究所
通讯作者Zhang, Lianmin; Zhang, Chunzhi
作者单位1.Shandong Univ Sci & Technol, Sch Mat Sci & Engn, Qingdao 266590, Peoples R China
2.Chinese Acad Sci, CAS Key Lab Nucl Mat & Safety Assessment, Inst Met Res, 62 Wencui Rd, Shenyang 110016, Peoples R China
推荐引用方式
GB/T 7714
Sun, Shengxuan,Zhang, Lianmin,Ma, Aili,et al. Comparison of the Three-Phase Corrosion Behavior of SiN and 304L Stainless Steels in 6 M Nitric Acid Solution at Different Temperatures[J]. METALS,2022,12(6):17.
APA Sun, Shengxuan,Zhang, Lianmin,Ma, Aili,Daniel, Enobong Felix,Zhang, Chunzhi,&Zheng, Yugui.(2022).Comparison of the Three-Phase Corrosion Behavior of SiN and 304L Stainless Steels in 6 M Nitric Acid Solution at Different Temperatures.METALS,12(6),17.
MLA Sun, Shengxuan,et al."Comparison of the Three-Phase Corrosion Behavior of SiN and 304L Stainless Steels in 6 M Nitric Acid Solution at Different Temperatures".METALS 12.6(2022):17.

入库方式: OAI收割

来源:金属研究所

浏览0
下载0
收藏0
其他版本

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。