Application of Modified Coke to NOx Reduction with Recycling Flue Gas during Iron Ore Sintering Process

文献类型:期刊论文

作者Chen, Yan-guang1,2; Guo, Zhan-cheng1,3; Wang, Zhi1
刊名ISIJ INTERNATIONAL
出版日期2008
卷号48期号:11页码:1517-1523
关键词iron ore sintering NOx modified coke recycled flue gas
ISSN号0915-1559
其他题名ISIJ Int.
中文摘要A new process, named NOx reduction by the modified coke with recycling flue gas, was proposed. The coke samples loaded with K2CO3, CaO and CeO2 were characterized by SEM. The effects of the recycled flue gas and the modified coke on NOx reduction were investigated with a quartz fixed bed reactor and a sintering pot. The results showed that the extent of the contact between additives and coke was: K2CO3>CaO>CeO2. In the modified coke combustion with recycling flue gas, the concentration of NOx emission was decreased, furthermore, the NO, reduction ratio increased with the loading amount of additives. The NO, reduction ratios were 36.7%, 20.2% and 26.2% respectively when the loading amount of K2CO3 CaO and CeO2 was 2.0%. In sintering pot tests, the coke loaded with 2.0% CeO2 was used as fuel and the recycled flue gas, simulated by the gas mixture with 50 ppm NO, was introduced to sintering process, the NO, reduction ratio was 38.0%, which was about 13% higher than that of the base run with recycling flue gas.
英文摘要A new process, named NOx reduction by the modified coke with recycling flue gas, was proposed. The coke samples loaded with K2CO3, CaO and CeO2 were characterized by SEM. The effects of the recycled flue gas and the modified coke on NOx reduction were investigated with a quartz fixed bed reactor and a sintering pot. The results showed that the extent of the contact between additives and coke was: K2CO3>CaO>CeO2. In the modified coke combustion with recycling flue gas, the concentration of NOx emission was decreased, furthermore, the NO, reduction ratio increased with the loading amount of additives. The NO, reduction ratios were 36.7%, 20.2% and 26.2% respectively when the loading amount of K2CO3 CaO and CeO2 was 2.0%. In sintering pot tests, the coke loaded with 2.0% CeO2 was used as fuel and the recycled flue gas, simulated by the gas mixture with 50 ppm NO, was introduced to sintering process, the NO, reduction ratio was 38.0%, which was about 13% higher than that of the base run with recycling flue gas.
WOS标题词Science & Technology ; Technology
类目[WOS]Metallurgy & Metallurgical Engineering
研究领域[WOS]Metallurgy & Metallurgical Engineering
关键词[WOS]NITRIC-OXIDE ; COMBUSTION ; COAL ; OXIDATION ; EMISSION ; CHAR ; CONVERSION ; CATALYST ; NITROGEN ; CARBON
收录类别SCI
原文出处://WOS:000262795000005
语种英语
WOS记录号WOS:000262795000005
公开日期2013-10-08
版本出版稿
源URL[http://ir.ipe.ac.cn/handle/122111/2727]  
专题过程工程研究所_研究所(批量导入)
作者单位1.Chinese Acad Sci, Inst Proc Engn, State Key Lab Multiphase Complex Syst, Beijing 100190, Peoples R China
2.Chinese Acad Sci, Grad Univ, Beijing 100049, Peoples R China
3.Univ Sci & Technol Beijing, Sch Met & Ecol Engn, Beijing 100083, Peoples R China
推荐引用方式
GB/T 7714
Chen, Yan-guang,Guo, Zhan-cheng,Wang, Zhi. Application of Modified Coke to NOx Reduction with Recycling Flue Gas during Iron Ore Sintering Process[J]. ISIJ INTERNATIONAL,2008,48(11):1517-1523.
APA Chen, Yan-guang,Guo, Zhan-cheng,&Wang, Zhi.(2008).Application of Modified Coke to NOx Reduction with Recycling Flue Gas during Iron Ore Sintering Process.ISIJ INTERNATIONAL,48(11),1517-1523.
MLA Chen, Yan-guang,et al."Application of Modified Coke to NOx Reduction with Recycling Flue Gas during Iron Ore Sintering Process".ISIJ INTERNATIONAL 48.11(2008):1517-1523.

入库方式: OAI收割

来源:过程工程研究所

浏览0
下载0
收藏0
其他版本

除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。