Achieving superior mechanical and corrosion properties in medium-thickness Ti-6Al-4 V alloy joints by back heating assisted friction stir welding below β-phase transformation temperature

文献类型:期刊论文

作者Cong, S.1,2; Wu, L. H.1,2; Wang, Z. W.1,2; Li, N.1,2; Zhu, Z.3; Wang, F. F.4; Zhang, X.5; Wang, K.5; Xue, P.1,2; Ni, D. R.1,2
刊名MATERIALS CHARACTERIZATION
出版日期2024-11-01
卷号217页码:11
关键词Ti alloys Friction stir welding Back heating assisting welding Microstructure Mechanical property Corrosion resistance
ISSN号1044-5803
DOI10.1016/j.matchar.2024.114391
通讯作者Wu, L. H.(lhwu@imr.ac.cn) ; Wang, Z. W.(zwwang16b@imr.ac.cn)
英文摘要The equiaxed microstructure formed below the beta-phase transition point of Ti alloys generally exhibits an excellent balance of mechanical properties and corrosion resistance. However, this desirable microstructure is impossible to be obtained in fusion welded joints but is prospective to be achieved by the solid-state friction stir welding (FSW) technique. Unfortunately, it generally generates bottom defects and severe tool wear in medium- thickness Ti alloy joints when conventional FSW was conducted below the beta-phase transition point. In this study, 6 mm thick Ti-6Al-4 V plates were joined by both the conventional FSW and back heating assisted FSW (BHAFSW). Defects caused by significant tool wear and bottom phase transition differences occurred in the conventional FSW. It was found that the hardness difference between the base material (BM) and the tool increased to 35.6 % from 500 degrees C to 900 degrees C. The back heating (150 degrees C) was used to control welding temperatures remaining the 900 degrees C, thus largely reducing the tool wear by increasing the hardness difference. In addition, the back temperature compensation increased the bottom temperature and controlled the phase transition position from the bottom to the middle of the joint. The shoulder pressure contributed to the compression of the defects, and the defects were eliminated by increasing the pressure at the phase transition position. A significantly refined equiaxed microstructure with an average grain size of similar to 0.9 mu m was achieved below the beta-phase transition temperature in the stir zone via back heating assisted FSW, while a bimodal structure with an average grain size of 3.5 mu m was formed near the beta-phase transition temperature. Inconspicuous reduction of the strength was detected for the joints (98 % of the BM) which possess equiaxed microstructures, and the corrosion resistance of the joints was enhanced compared to the BM. This superior synergy of mechanical and corrosion properties exceeded the majority of Ti alloy joints previously reported. This study provided an effective method for obtaining medium-thickness Ti alloy joints with ultrafine equiaxial structures with superior mechanical properties and corrosion resistance.
资助项目National Natural Science Foundation of China[52171057] ; National Natural Science Foundation of China[52301067] ; Youth Innovation Promotion Association of the Chinese Academy of Sciences[2021193] ; Youth Innovation Promotion Association of the Chinese Academy of Sciences[Y2021061] ; Shi Changxu Innovation Center for Advanced Materials[SCXKFJJ202210]
WOS研究方向Materials Science ; Metallurgy & Metallurgical Engineering
语种英语
WOS记录号WOS:001334994100001
出版者ELSEVIER SCIENCE INC
资助机构National Natural Science Foundation of China ; Youth Innovation Promotion Association of the Chinese Academy of Sciences ; Shi Changxu Innovation Center for Advanced Materials
源URL  
专题金属研究所_中国科学院金属研究所
通讯作者Wu, L. H.; Wang, Z. W.
作者单位1.Chinese Acad Sci, Inst Met Res, Shi Changxu Innovat Ctr Adv Mat, 72 Wenhua Rd, Shenyang 110016, Peoples R China
2.Univ Sci & Technol China, Sch Mat Sci & Engn, 72 Wenhua Rd, Shenyang 110016, Peoples R China
3.Shenyang Aerosp Univ, Coll Mat Sci & Engn, 37 Daoyi South Ave, Shenyang 110136, Peoples R China
4.China Acad Launch Vehicle Technol, Beijing 100076, Peoples R China
5.Capital Aerosp Machinery Co Ltd, 2 Jingbei East Rd, Beijing 100076, Peoples R China
推荐引用方式
GB/T 7714
Cong, S.,Wu, L. H.,Wang, Z. W.,et al. Achieving superior mechanical and corrosion properties in medium-thickness Ti-6Al-4 V alloy joints by back heating assisted friction stir welding below β-phase transformation temperature[J]. MATERIALS CHARACTERIZATION,2024,217:11.
APA Cong, S..,Wu, L. H..,Wang, Z. W..,Li, N..,Zhu, Z..,...&Ma, Z. Y..(2024).Achieving superior mechanical and corrosion properties in medium-thickness Ti-6Al-4 V alloy joints by back heating assisted friction stir welding below β-phase transformation temperature.MATERIALS CHARACTERIZATION,217,11.
MLA Cong, S.,et al."Achieving superior mechanical and corrosion properties in medium-thickness Ti-6Al-4 V alloy joints by back heating assisted friction stir welding below β-phase transformation temperature".MATERIALS CHARACTERIZATION 217(2024):11.

入库方式: OAI收割