Spark Plasma Sintering of Diamond Binderless WC Composites
文献类型:期刊论文
作者 | Yoshio Sakka |
刊名 | J. Am. Ceram. Soc.
![]() |
出版日期 | 2012 |
卷号 | 12期号:95页码:2423—2428 |
通讯作者 | Yoshio Sakka |
合作状况 | 李雨桐 |
中文摘要 | A new method was developed to fully consolidate binderless tungsten carbide and diamond powders by means of spark plasma sintering (SPS) in current-control mode (CCm). Below 900°C, the 2 cm diameter sample was slowly heated by a dc current of 1000 A. Above 900°C the imposed current was suddenly raised to 4000 A. The combination of the relatively high heating rate of 2000°C/min and the relatively short holding time of 1.5 min (above 1300°C) was successful to fabricate fully dense binderless WC/diamond composite. No graphitization of diamond was detected after ultrafast sintering as confirmed by optical and SEM microstructure observations, XRD and Raman analysis. The sample showed very high wear resistance in comparison to fully dense monolithic binderless WC compacts. The developed method, unlike previously published works, did not require any diamond coating to prevent diamond graphitization. I. Introduction |
学科主题 | 材料科学 |
原文出处 | SCI收录 |
公开日期 | 2013-12-16 |
源URL | [http://ir.nimte.ac.cn/handle/174433/9535] ![]() |
专题 | 宁波材料技术与工程研究所_宁波所知识产出 |
推荐引用方式 GB/T 7714 | Yoshio Sakka. Spark Plasma Sintering of Diamond Binderless WC Composites[J]. J. Am. Ceram. Soc.,2012,12(95):2423—2428. |
APA | Yoshio Sakka.(2012).Spark Plasma Sintering of Diamond Binderless WC Composites.J. Am. Ceram. Soc.,12(95),2423—2428. |
MLA | Yoshio Sakka."Spark Plasma Sintering of Diamond Binderless WC Composites".J. Am. Ceram. Soc. 12.95(2012):2423—2428. |
入库方式: OAI收割
来源:宁波材料技术与工程研究所
浏览0
下载0
收藏0
其他版本
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。