Critical silicon-anode size for averting lithiation-induced mechanical failure of lithium-ion batteries
文献类型:期刊论文
作者 | Ma ZS ; Li TT ; Huang YL ; Liu J ; Zhou YC ; Xue DF |
刊名 | rsc advances
![]() |
出版日期 | 2013 |
卷号 | 3期号:20页码:7398-7402 |
关键词 | THIN-FILM ANODE ELECTROCHEMICAL LITHIATION DEPENDENT FRACTURE ELECTRODES NANOSTRUCTURES INSERTION |
ISSN号 | 2046-2069 |
通讯作者 | ma zs |
中文摘要 | silicon nanostructures have been employed as the anodes of lithium-ion batteries to mitigate mechanical and chemical degradation. conditions for averting fracture have been identified in terms of the si critical size and its state of charge. strong size dependencies were observed, and the critical sizes of fracture for different shapes of si have been found to be: similar to 90 nm for nanoparticles, similar to 70 nm for nanowires, and similar to 33 nm for nanofilms, below which the silicon nanostructures remain undamaged upon lithiation. |
收录类别 | SCI收录期刊论文 |
语种 | 英语 |
WOS记录号 | WOS:000318302900035 |
公开日期 | 2014-04-18 |
源URL | [http://ir.ciac.jl.cn/handle/322003/50300] ![]() |
专题 | 长春应用化学研究所_长春应用化学研究所知识产出_期刊论文 |
推荐引用方式 GB/T 7714 | Ma ZS,Li TT,Huang YL,et al. Critical silicon-anode size for averting lithiation-induced mechanical failure of lithium-ion batteries[J]. rsc advances,2013,3(20):7398-7402. |
APA | Ma ZS,Li TT,Huang YL,Liu J,Zhou YC,&Xue DF.(2013).Critical silicon-anode size for averting lithiation-induced mechanical failure of lithium-ion batteries.rsc advances,3(20),7398-7402. |