A novel method to extract iron, titanium, vanadium, and chromium from high-chromium vanadium-bearing titanomagnetite concentrates
文献类型:期刊论文
作者 | Zhao, Longsheng1,2,3; Wang, Lina1,2; Qi, Tao1,2; Chen, Desheng1,2; Zhao, Hongxin1,2; Liu, Yahui1,2 |
刊名 | HYDROMETALLURGY
![]() |
出版日期 | 2014-10-01 |
卷号 | 149页码:106-109 |
关键词 | Titanomagnetite concentrates Partial reduction Hydrochloric acid leaching Alkaline desilication Titanium-rich slag |
ISSN号 | 0304-386X |
其他题名 | Hydrometallurgy |
中文摘要 | A novel process for the extraction of iron, titanium, vanadium, and chromium from high-chromium vanadium-bearing titanomagnetite concentrates is proposed. This process involves several steps: partial reduction of the concentrates, magnetic separation, hydrochloric acid leaching of the titanium-bearing tailing, and alkaline desilication of the HCl leach residue. The partial reduction ensures that the vanadium and chromium are predominantly concentrated in the titanium-bearing tailing. Subsequently, magnetic separation is used to recover an iron concentrate with a total iron content of 94.57%. During add treatment, 90.8% vanadium leaching and 93.4% chromium leaching were obtained, with titanium losses of less than 0.3%, 96.3% of the silicon was removed by alkaline desilication, and titanium-rich slag with a purity of 93.39% was produced. The total recoveries of iron, titanium, vanadium, and chromium under the experimental conditions were 88.3%, 93.7%, 81.7%, and 84.4%, respectively. (C) 2014 Elsevier B.V. All rights reserved. |
英文摘要 | A novel process for the extraction of iron, titanium, vanadium, and chromium from high-chromium vanadium-bearing titanomagnetite concentrates is proposed. This process involves several steps: partial reduction of the concentrates, magnetic separation, hydrochloric acid leaching of the titanium-bearing tailing, and alkaline desilication of the HCl leach residue. The partial reduction ensures that the vanadium and chromium are predominantly concentrated in the titanium-bearing tailing. Subsequently, magnetic separation is used to recover an iron concentrate with a total iron content of 94.57%. During add treatment, 90.8% vanadium leaching and 93.4% chromium leaching were obtained, with titanium losses of less than 0.3%, 96.3% of the silicon was removed by alkaline desilication, and titanium-rich slag with a purity of 93.39% was produced. The total recoveries of iron, titanium, vanadium, and chromium under the experimental conditions were 88.3%, 93.7%, 81.7%, and 84.4%, respectively. (C) 2014 Elsevier B.V. All rights reserved. |
WOS标题词 | Science & Technology ; Technology |
类目[WOS] | Metallurgy & Metallurgical Engineering |
研究领域[WOS] | Metallurgy & Metallurgical Engineering |
关键词[WOS] | BLAST-FURNACE SLAG ; HYDROCHLORIC-ACID ; DYNAMIC OXIDATION ; ROSETTA ILMENITE ; SYNTHETIC RUTILE ; MIXED PELLETS ; STEEL SLAG ; REDUCTION ; RECOVERY ; NA2CO3 |
收录类别 | SCI |
原文出处 | |
语种 | 英语 |
WOS记录号 | WOS:000344204400012 |
公开日期 | 2015-04-01 |
源URL | [http://ir.ipe.ac.cn/handle/122111/11901] ![]() |
专题 | 过程工程研究所_研究所(批量导入) |
作者单位 | 1.Natl Engn Lab Hydromet Cleaner Prod Technol, Beijing 100190, Peoples R China 2.Chinese Acad Sci, Inst Proc Engn, Key Lab Green Proc & Engn, Beijing 100190, Peoples R China 3.Univ Chinese Acad Sci, Beijing 100049, Peoples R China |
推荐引用方式 GB/T 7714 | Zhao, Longsheng,Wang, Lina,Qi, Tao,et al. A novel method to extract iron, titanium, vanadium, and chromium from high-chromium vanadium-bearing titanomagnetite concentrates[J]. HYDROMETALLURGY,2014,149:106-109. |
APA | Zhao, Longsheng,Wang, Lina,Qi, Tao,Chen, Desheng,Zhao, Hongxin,&Liu, Yahui.(2014).A novel method to extract iron, titanium, vanadium, and chromium from high-chromium vanadium-bearing titanomagnetite concentrates.HYDROMETALLURGY,149,106-109. |
MLA | Zhao, Longsheng,et al."A novel method to extract iron, titanium, vanadium, and chromium from high-chromium vanadium-bearing titanomagnetite concentrates".HYDROMETALLURGY 149(2014):106-109. |
入库方式: OAI收割
来源:过程工程研究所
浏览0
下载0
收藏0
其他版本
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。