Preparation of Ti-enriched slag from V-bearing titanomagnetite by two-stage hydrochloric acid leaching route
文献类型:期刊论文
作者 | Zhong, Binnian1,2; Xue, Tianyan1; Zhao, Longsheng1; Zhao, Hongxin1; Qi, Tao1; Chen, Weiliang2 |
刊名 | SEPARATION AND PURIFICATION TECHNOLOGY
![]() |
出版日期 | 2014-11-24 |
卷号 | 137期号:NOV.页码:59-65 |
关键词 | V-Ti concentrate Hydrochloric acid leaching Molecular simulation Impurity separation Ti-enriched slag |
ISSN号 | 1383-5866 |
其他题名 | Sep. Purif. Technol. |
中文摘要 | Low-grade, highly reactive V-Ti concentrate was obtained from V-bearing titanomagnetite via selective reduction-magnetic separation. The main phases of the concentrate are anosovite and pyroxene. Two-stage acid leaching was employed to remove the impurities in the concentrate. The leaching behavior of impurities Ca/Mg/Al/Si under different acid leaching conditions in the first stage was investigated in detail. The optimal leaching conditions of the first-stage were as follows: 383 K leaching temperature, 1.40 mol/L HCl concentration, 1/10 solid-liquid mass ratio, and 120 min leaching time, under which the residue obtained contained 79.54% of TiO2 and 2.50% of V2O5. The result of molecular structure simulation indicate that the Ti-O and Mg-O bonds in the anosovite phase are broken under oxygen pressure conditions in the second stage by reacted with HCl solution. The content of TiO2 in the Ti-enriched slag prepared by two-stage acid leaching can reach 92.5% with further removal of residual carbon. (C) 2014 Elsevier B.V. All rights reserved. |
英文摘要 | Low-grade, highly reactive V-Ti concentrate was obtained from V-bearing titanomagnetite via selective reduction-magnetic separation. The main phases of the concentrate are anosovite and pyroxene. Two-stage acid leaching was employed to remove the impurities in the concentrate. The leaching behavior of impurities Ca/Mg/Al/Si under different acid leaching conditions in the first stage was investigated in detail. The optimal leaching conditions of the first-stage were as follows: 383 K leaching temperature, 1.40 mol/L HCl concentration, 1/10 solid-liquid mass ratio, and 120 min leaching time, under which the residue obtained contained 79.54% of TiO2 and 2.50% of V2O5. The result of molecular structure simulation indicate that the Ti-O and Mg-O bonds in the anosovite phase are broken under oxygen pressure conditions in the second stage by reacted with HCl solution. The content of TiO2 in the Ti-enriched slag prepared by two-stage acid leaching can reach 92.5% with further removal of residual carbon. (C) 2014 Elsevier B.V. All rights reserved. |
WOS标题词 | Science & Technology ; Technology |
类目[WOS] | Engineering, Chemical |
研究领域[WOS] | Engineering |
关键词[WOS] | TITANIUM-DIOXIDE ; ILMENITE |
收录类别 | SCI |
原文出处 | |
语种 | 英语 |
WOS记录号 | WOS:000345181500008 |
公开日期 | 2015-04-01 |
源URL | [http://ir.ipe.ac.cn/handle/122111/11905] ![]() |
专题 | 过程工程研究所_研究所(批量导入) |
作者单位 | 1.Chinese Acad Sci, Inst Proc Engn, Key Lab Green Proc & Engn, Beijing 100190, Peoples R China 2.Kunming Univ Sci & Technol, Fac Met & Energy Engn, Natl Engn Lab Vacuum Met, Kunming 650093, Peoples R China |
推荐引用方式 GB/T 7714 | Zhong, Binnian,Xue, Tianyan,Zhao, Longsheng,et al. Preparation of Ti-enriched slag from V-bearing titanomagnetite by two-stage hydrochloric acid leaching route[J]. SEPARATION AND PURIFICATION TECHNOLOGY,2014,137(NOV.):59-65. |
APA | Zhong, Binnian,Xue, Tianyan,Zhao, Longsheng,Zhao, Hongxin,Qi, Tao,&Chen, Weiliang.(2014).Preparation of Ti-enriched slag from V-bearing titanomagnetite by two-stage hydrochloric acid leaching route.SEPARATION AND PURIFICATION TECHNOLOGY,137(NOV.),59-65. |
MLA | Zhong, Binnian,et al."Preparation of Ti-enriched slag from V-bearing titanomagnetite by two-stage hydrochloric acid leaching route".SEPARATION AND PURIFICATION TECHNOLOGY 137.NOV.(2014):59-65. |
入库方式: OAI收割
来源:过程工程研究所
浏览0
下载0
收藏0
其他版本
除非特别说明,本系统中所有内容都受版权保护,并保留所有权利。