条数/页: 排序方式:
The microstructure and mechanical performance optimization of a new Fe-Ni-based superalloy for Gen IV nuclear reactor: The critical role of Nb alloying strategy 期刊论文  OAI收割
MATERIALS CHARACTERIZATION, 2023, 卷号: 205, 页码: 15
作者:  
Wang, Jiaqi;  Qin, Xuezhi;  Cheng, Sihan;  Guan, Xianjun;  Zhou, Lanzhang
  |  收藏  |  浏览/下载:8/0  |  提交时间:2024/01/07
Effect of cold rolling on microstructure, texture, and tensile properties of a Ni-Fe-based superalloy 期刊论文  OAI收割
JOURNAL OF ALLOYS AND COMPOUNDS, 2023, 卷号: 937, 页码: 14
作者:  
Wang, Jiaqi;  Cheng, Sihan;  Wu, Yunsheng;  Wang, Tingting;  Qin, Xuezhi
  |  收藏  |  浏览/下载:48/0  |  提交时间:2023/05/09
Microstructure, thermal stability and tensile properties of a Ni-Fe-Cr based superalloy with different Fe contents 期刊论文  OAI收割
INTERMETALLICS, 2023, 卷号: 153, 页码: 12
作者:  
Cheng, Sihan;  Wang, Jiaqi;  Wu, Yunsheng;  Qin, Xuezhi;  Zhou, Lanzhang
  |  收藏  |  浏览/下载:22/0  |  提交时间:2023/05/09
Coherent precipitation and stability of cuboidal B2 nanoparticles in a ferritic Fe-Cr-Ni-Al superalloy 期刊论文  OAI收割
MATERIALS RESEARCH LETTERS, 2021, 卷号: 9, 期号: 11, 页码: 458-466
作者:  
Wang, Zhenhua;  Wang, Qing;  Niu, Ben;  Dong, Chuang;  Zhang, Hongwei
  |  收藏  |  浏览/下载:93/0  |  提交时间:2021/11/22
Effects of nitrogen content on microstructures and tensile properties of a new Ni-Fe based wrought superalloy 期刊论文  OAI收割
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 卷号: 801, 页码: 10
作者:  
Liu, Peng;  Zhang, Rui;  Yuan, Yong;  Cui, Chuanyong;  Liang, Faguang
  |  收藏  |  浏览/下载:43/0  |  提交时间:2021/03/15
Microstructures and intermediate temperature brittleness of newly developed Ni-Fe based weld metal for ultra-supercritical power plants 期刊论文  OAI收割
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 卷号: 684, 页码: 146-157
Wu, Dong; Li, Dianzhong; Lu, Shanping
收藏  |  浏览/下载:80/0  |  提交时间:2017/08/17
Microstructural stability and mechanical properties of a boron modified Ni-Fe based superalloy for steam boiler applications 期刊论文  OAI收割
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 卷号: 639, 页码: 380-388
Wang, Changshuai; Guo, YongAn; Guo, Jianting; Zhou, Lanzhang
收藏  |  浏览/下载:27/0  |  提交时间:2016/04/21
A Newly Developed Wrought Ni-Fe-Cr-based Superalloy for Advanced Ultra-Supercritical Power Plant Applications Beyond 700 degrees C 期刊论文  OAI收割
ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2015, 卷号: 28, 期号: 9, 页码: 1083-1088
Guan, Shuai; Cui, Chuan-Yong
收藏  |  浏览/下载:13/0  |  提交时间:2016/04/21
Thermal Stability of a New Ni-Fe-Cr Base Alloy with Different Ti/Al Ratios 期刊论文  OAI收割
Journal of Materials Science & Technology, 2015, 卷号: 31, 期号: 2, 页码: 135-142
C. S.; Wang Wang, T. T.; Tan, M. L.; Guo, Y. G.; Guo, J. T.; Zhou, L. Z.
收藏  |  浏览/下载:27/0  |  提交时间:2015/05/08
A Newly Developed Wrought Ni–Fe–Cr-based Superalloy for Advanced Ultra-Supercritical Power Plant Applications Beyond 700 °C 期刊论文  OAI收割
Acta Metallurgica Sinica(English Letters), 2015, 卷号: 28, 期号: 9, 页码: 1083-1088
作者:  
Guan Shuai;  Cui Chuanyong
  |  收藏  |  浏览/下载:16/0  |  提交时间:2021/02/02