Comprehensive damage and deformation mechanisms during out-of-phase thermal mechanical fatigue of the fourth-generation single crystal superalloy 期刊论文  OAI收割
INTERNATIONAL JOURNAL OF FATIGUE, 2024, 卷号: 178, 页码: 14
作者:  
Tan, Zihao;  Wang, Xinguang;  Li, Yongmei;  Yang, Yanhong;  Du, Yunling
  |  收藏  |  浏览/下载:24/0  |  提交时间:2024/01/07
Pore-induced defects during thermo-mechanical fatigue of a fourth-generation single crystal superalloy 期刊论文  OAI收割
MATERIALS RESEARCH LETTERS, 2023, 卷号: 11, 期号: 8, 页码: 678-687
作者:  
Tan, Zihao;  Wang, Xinguang;  Pang, Jianchao;  Zou, Mingke;  Tao, Yan
  |  收藏  |  浏览/下载:15/0  |  提交时间:2024/01/07