中国科学院机构知识库网格
Chinese Academy of Sciences Institutional Repositories Grid
机构
采集方式
内容类型
发表日期
学科主题
筛选

浏览/检索结果: 共41条,第1-10条 帮助

条数/页: 排序方式:
Microstructure evolutions and deformation mechanisms of a Ni-based GH3536 Superalloy during loading at 293 K and 77 K 期刊论文  OAI收割
MATERIALS CHARACTERIZATION, 2023, 卷号: 206, 页码: 13
作者:  
Wang, Yong-Qiang;  Yuan, Chao;  Zhang, Bing;  Gao, Xin-Yu;  Qiao, Shi-Chang
  |  收藏  |  浏览/下载:22/0  |  提交时间:2024/01/07
Insights into stress corrosion cracking in scratched area of alloy 690TT steam generator tubes 期刊论文  OAI收割
ACTA MATERIALIA, 2023, 卷号: 255, 页码: 16
作者:  
Wu, Bin;  Zhang, Yusheng;  Meng, Fanjiang;  Zhang, Zhiming;  Li, Yifeng
  |  收藏  |  浏览/下载:9/0  |  提交时间:2024/01/07
The effect of porosity size and oxidation on the HCF property of nickel-based single crystal superalloy at 980 degrees C 期刊论文  OAI收割
THEORETICAL AND APPLIED FRACTURE MECHANICS, 2022, 卷号: 120, 页码: 16
作者:  
Jiang, Wen;  Li, Piao;  Yao, Wei-Xing;  Rui, Shao-Shi;  Shi, Hui-Ji
  |  收藏  |  浏览/下载:46/0  |  提交时间:2022/08/02
Effect of solution heat treatment on creep properties of a nickel-based single crystal superalloy 期刊论文  OAI收割
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2021, 卷号: 15, 页码: 4702-4713
作者:  
Yunling, Du;  Yang, Yanhong;  Diao, Aimin;  Li, Yongmei;  Wang, Xinguang
  |  收藏  |  浏览/下载:92/0  |  提交时间:2022/01/27
A new refractory Ni7Nb2 phase identified in Laves eutectic regions by TEM study 期刊论文  OAI收割
ACTA MATERIALIA, 2021, 卷号: 214, 页码: 10
作者:  
Ge, Hualong;  Xing, Weiwei;  Chen, Bo;  Hu, Xiaobing;  Zheng, Shijian
  |  收藏  |  浏览/下载:44/0  |  提交时间:2021/10/15
Creep behavior and a deformation mechanism based creep rate model under high temperature and low stress condition for single crystal superalloy DD5 期刊论文  OAI收割
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 卷号: 786, 页码: 10
作者:  
Xu, Ke;  Wang, Guanglei;  Liu, Jide;  Li, Jinguo;  Liu, Jinlai
  |  收藏  |  浏览/下载:47/0  |  提交时间:2021/02/02
Microstructural modification and mechanical characterization for a laser-induced composite coating during thermal exposure 期刊论文  OAI收割
SURFACE & COATINGS TECHNOLOGY, 2019, 卷号: 358, 页码: 11-21
作者:  
He, Yanming;  Lu, Chuanyang;  Zheng, Wenjian;  Yang, Jianguo;  Chen, Shuangjian
  |  收藏  |  浏览/下载:31/0  |  提交时间:2021/02/02
Microstructural modification and mechanical characterization for a laser-induced composite coating during thermal exposure 期刊论文  OAI收割
SURFACE & COATINGS TECHNOLOGY, 2019, 卷号: 358, 页码: 11-21
作者:  
He, Yanming;  Lu, Chuanyang;  Zheng, Wenjian;  Yang, Jianguo;  Chen, Shuangjian
  |  收藏  |  浏览/下载:17/0  |  提交时间:2021/02/02
Comprehensive first-principles study of transition-metal substitution in the gamma phase of nickel-based superalloys 期刊论文  OAI收割
CALPHAD-COMPUTER COUPLING OF PHASE DIAGRAMS AND THERMOCHEMISTRY, 2018, 卷号: 61, 页码: 41-49
作者:  
Chen, WL;  Xing, WW;  Ma, H;  Ding, XY;  Chen, XQ
  |  收藏  |  浏览/下载:55/0  |  提交时间:2018/12/25
Comprehensive first-principles study of transition-metal substitution in the gamma phase of nickel-based superalloys 期刊论文  OAI收割
CALPHAD-COMPUTER COUPLING OF PHASE DIAGRAMS AND THERMOCHEMISTRY, 2018, 卷号: 61, 页码: 41-49
作者:  
Chen, Weiliang;  Xing, Weiwei;  Ma, Hui;  Ding, Xueyong;  Chen, Xing-Qiu
  |  收藏  |  浏览/下载:14/0  |  提交时间:2021/02/02