中国科学院机构知识库网格
Chinese Academy of Sciences Institutional Repositories Grid
首页
机构
成果
学者
登录
注册
登陆
×
验证码:
换一张
忘记密码?
记住我
×
校外用户登录
CAS IR Grid
机构
金属研究所 [28]
采集方式
OAI收割 [28]
内容类型
期刊论文 [27]
学位论文 [1]
发表日期
2023 [1]
2022 [3]
2021 [2]
2020 [3]
2019 [2]
2014 [2]
更多
学科主题
筛选
浏览/检索结果:
共28条,第1-10条
帮助
条数/页:
5
10
15
20
25
30
35
40
45
50
55
60
65
70
75
80
85
90
95
100
排序方式:
请选择
提交时间升序
提交时间降序
作者升序
作者降序
题名升序
题名降序
发表日期升序
发表日期降序
Effect of strain rate on microstructure evolution of a fine-grained gamma plus gamma' Ni-Co-base superalloy during superplasticity
期刊论文
OAI收割
MATERIALS CHARACTERIZATION, 2023, 卷号: 203, 页码: 13
作者:
Al-Hammadi, Rashad A.
;
Zhang, Rui
;
Cui, Chuanyong
;
Zhou, Zijian
;
Zhou, Yizhou
  |  
收藏
  |  
浏览/下载:21/0
  |  
提交时间:2024/01/08
Ni-Co-base superalloy
Superplasticity
Microstructure evolution
gamma'-phase
Twin
Influence of solution temperature on microstructure and creep behaviors of a Ni-Co base superalloy for turbine disc
期刊论文
OAI收割
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 卷号: 853, 页码: 13
作者:
Zhou, Zijian
;
Zhang, Rui
;
Cui, Chuanyong
;
Zhou, Yizhou
;
Sun, Xiaofeng
  |  
收藏
  |  
浏览/下载:28/0
  |  
提交时间:2023/05/09
Ni-Co base Superalloy
Solution temperature
Grain boundary character distribution
Carbide morphology
Creep behavior
Effect of pre-strain treatment on mechanical properties of a Ni-Co base disk superalloy
期刊论文
OAI收割
JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 卷号: 905, 页码: 10
作者:
Zhu, C. Z.
;
Zhang, R.
  |  
收藏
  |  
浏览/下载:62/0
  |  
提交时间:2022/07/01
Ni-Co base superalloy
Pre-strain
Microstructure
Mechanical property
Microtwinning
Suzuki segregation
Evolution of Interfacial Microstructure of Ni-Co Base Superalloy During Plastic Deformation Bonding and Its Bonding Mechanism
期刊论文
OAI收割
ACTA METALLURGICA SINICA, 2022, 卷号: 58, 期号: 2, 页码: 129-140
作者:
Ren Shaofei
;
Zhang Jianyang
;
Zhang Xinfang
;
Sun Mingyue
;
Xu Bin
  |  
收藏
  |  
浏览/下载:65/0
  |  
提交时间:2022/07/01
Ni-Co base superalloy
plastic deformation bonding
dynamic recrystallization
Influence of Ta content on microstructure and creep behavior of a Ni-Co base disc superalloy
期刊论文
OAI收割
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 卷号: 802, 页码: 10
作者:
Zhu, C. Z.
;
Zhang, R.
;
Cui, C. Y.
;
Zhou, Y. Z.
;
Liang, F. G.
  |  
收藏
  |  
浏览/下载:53/0
  |  
提交时间:2021/10/15
Ni-Co base superalloy
Tantalum
Microstructure
Creep behavior
Influence of Ta content on microstructure and creep behavior of a Ni-Co base disc superalloy
期刊论文
OAI收割
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 卷号: 802, 页码: 10
作者:
Zhu, C. Z.
;
Zhang, R.
;
Cui, C. Y.
;
Zhou, Y. Z.
;
Liang, F. G.
  |  
收藏
  |  
浏览/下载:42/0
  |  
提交时间:2021/10/15
Ni-Co base superalloy
Tantalum
Microstructure
Creep behavior
Intergrowth structure of Laves within mu phases in Co-Al-W base superalloy
期刊论文
OAI收割
JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 卷号: 844, 页码: 8
作者:
Liu, L. R.
;
Zhou, B. X.
;
Wang, Q. F.
;
Yang, Y. H.
;
Yu, J. J.
  |  
收藏
  |  
浏览/下载:95/0
  |  
提交时间:2021/02/02
Co-Al-W base Superalloy
Topologically close-packed phases
Intergrowth
Quaternary compounds
Substitution
Intergrowth structure of Laves within mu phases in Co-Al-W base superalloy
期刊论文
OAI收割
JOURNAL OF ALLOYS AND COMPOUNDS, 2020, 卷号: 844, 页码: 8
作者:
Liu, L. R.
;
Zhou, B. X.
;
Wang, Q. F.
;
Yang, Y. H.
;
Yu, J. J.
  |  
收藏
  |  
浏览/下载:95/0
  |  
提交时间:2021/02/02
Co-Al-W base Superalloy
Topologically close-packed phases
Intergrowth
Quaternary compounds
Substitution
Influence of Co content on the microstructures and mechanical properties of a Ni-Co base superalloy made by specific additive manufacturing process
期刊论文
OAI收割
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 卷号: 786, 页码: 10
作者:
Tang, Ling
;
Liang, Jingjing
;
Cui, Chuanyong
;
Li, Jinguo
;
Zhou, Yizhou
  |  
收藏
  |  
浏览/下载:33/0
  |  
提交时间:2021/02/02
Additive manufacturing
Ni-Co base Superalloy
Tensile strength
Deformation mechanism
Borides of preferred orientation formed in the transient liquid phase joint of gamma '-strengthened Co-base single crystal superalloy
期刊论文
OAI收割
MATERIALS LETTERS, 2019, 卷号: 246, 页码: 190-194
作者:
Wang, S. Y.
;
Sun, Y.
;
Hou, X. Y.
;
Cui, C. Y.
;
Sun, X. F.
  |  
收藏
  |  
浏览/下载:20/0
  |  
提交时间:2021/02/02
Transient liquid phase
gamma '-Strengthened Co-base superalloy
Boride of preferred orientation
Diffusion
Crystal growth