Microstructural evolution and fatigue cracking mechanisms of as-built and solution-aged Inconel 718 superalloy fabricated by selective laser melting at service temperature 期刊论文  OAI收割
ENGINEERING FAILURE ANALYSIS, 2025, 卷号: 181, 页码: 18
作者:  
Sun, Chuanwen;  Li, Wei;  Li, Cheng;  Cao, Xiaobo;  Sun, Rui
  |  收藏  |  浏览/下载:21/0  |  提交时间:2025/11/03
Fatigue-induced microstructural deformation and multimode defect-assisted cracking of laser powder bed fused superalloy at 650 °C 期刊论文  OAI收割
INTERMETALLICS, 2025, 卷号: 185, 页码: 15
作者:  
Sun, Chuanwen;  Li, Wei;  Serjouei, Ahmad;  Cao, Xiaobo;  Li C(李成)
  |  收藏  |  浏览/下载:33/0  |  提交时间:2025/09/08
Evolution behavior of competing fatigue failure and life prediction related to defect, stress and temperature for laser powder bed fused superalloy with solution aging treatment 期刊论文  OAI收割
INTERNATIONAL JOURNAL OF FATIGUE, 2025, 卷号: 198, 页码: 17
作者:  
Sun, Chuanwen;  Li, Wei;  Liu, Gang;  Sun, Rui;  Wang, Chuanpeng
  |  收藏  |  浏览/下载:51/0  |  提交时间:2025/07/22
Evolution of residual stress and microstructure in single crystal superalloys via directed energy deposition 期刊论文  OAI收割
OPTICS AND LASER TECHNOLOGY, 2025, 卷号: 186, 页码: 12
作者:  
Guo, Yimo;  Lu, Nannan;  Yang, Yanhong;  Liang, Jingjing;  Zhang, Guangrui
  |  收藏  |  浏览/下载:3/0  |  提交时间:2025/04/27
Evolution of residual stress and microstructure in single crystal superalloys via directed energy deposition 期刊论文  OAI收割
OPTICS AND LASER TECHNOLOGY, 2025, 卷号: 186, 页码: 12
作者:  
Guo, Yimo;  Lu, Nannan;  Yang, Yanhong;  Liang, Jingjing;  Zhang, Guangrui
  |  收藏  |  浏览/下载:3/0  |  提交时间:2025/04/27
Evolution of residual stress and microstructure in single crystal superalloys via directed energy deposition 期刊论文  OAI收割
OPTICS AND LASER TECHNOLOGY, 2025, 卷号: 186, 页码: 12
作者:  
Guo, Yimo;  Lu, Nannan;  Yang, Yanhong;  Liang, Jingjing;  Zhang, Guangrui
  |  收藏  |  浏览/下载:2/0  |  提交时间:2025/04/27
Evolution of residual stress and microstructure in single crystal superalloys via directed energy deposition 期刊论文  OAI收割
OPTICS AND LASER TECHNOLOGY, 2025, 卷号: 186, 页码: 12
作者:  
Guo, Yimo;  Lu, Nannan;  Yang, Yanhong;  Liang, Jingjing;  Zhang, Guangrui
  |  收藏  |  浏览/下载:2/0  |  提交时间:2025/04/27
The effect of secondary dendrite orientation on thickness debit effect of nickel-based single-crystal superalloy with tubular samples 期刊论文  OAI收割
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2025, 卷号: 217, 页码: 80-92
作者:  
Liu, Jing;  Yu, Minghan;  Min, Shiling;  Zhang, Gong;  Xu, Zhengguo
  |  收藏  |  浏览/下载:2/0  |  提交时间:2025/04/27
Dynamic recovery and recrystallization of an as-cast SX superalloy during hot deformation 期刊论文  OAI收割
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2025, 卷号: 217, 页码: 296-310
作者:  
Li, Yihang;  Jiang, Zhipeng;  Li, Longfei
  |  收藏  |  浏览/下载:3/0  |  提交时间:2025/04/27
Dynamic recovery and recrystallization of an as-cast SX superalloy during hot deformation 期刊论文  OAI收割
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2025, 卷号: 217, 页码: 296-310
作者:  
Li, Yihang;  Jiang, Zhipeng;  Li, Longfei;  Xie, Guang;  Zhang, Jian
  |  收藏  |  浏览/下载:3/0  |  提交时间:2025/04/27