中国科学院机构知识库网格
Chinese Academy of Sciences Institutional Repositories Grid
机构
采集方式
内容类型
发表日期
学科主题
筛选

浏览/检索结果: 共4条,第1-4条 帮助

条数/页: 排序方式:
Effects of gamma '-precipitate coarseningon tensile properties of Ni base superalloy K44 during long-term aging 期刊论文  OAI收割
ACTA METALLURGICA SINICA, 2006, 卷号: 42, 期号: 5, 页码: 481-486
作者:  
Hou, JS;  Guo, JT;  Zhou, LZ;  Ye, HQ
  |  收藏  |  浏览/下载:14/0  |  提交时间:2021/02/02
Effects of gamma '-precipitate coarseningon tensile properties of Ni base superalloy K44 during long-term aging 期刊论文  OAI收割
ACTA METALLURGICA SINICA, 2006, 卷号: 42, 期号: 5, 页码: 481-486
作者:  
Hou, JS;  Guo, JT;  Zhou, LZ;  Ye, HQ
  |  收藏  |  浏览/下载:27/0  |  提交时间:2021/02/02
Prediction and improvement of mechanical properties of corrosion resistant superalloy K44 with adjusting minor additions C, B and Hf 期刊论文  OAI收割
Materials Transactions, 2006, 卷号: 47, 期号: 1, 页码: 198-206
J. T. Guo; J. S. Hou; L. Z. Zhou; H. Q. Ye
收藏  |  浏览/下载:32/0  |  提交时间:2012/04/13
Isothermal oxidation behavior of cast Ni-base superalloy K44 期刊论文  OAI收割
Transactions of Nonferrous Metals Society of China, 2006, 卷号: 16, 页码: S1967-S1972
Y. Li; X. G. Liu; J. T. Guo; C. Yuan; H. C. Yang
收藏  |  浏览/下载:26/0  |  提交时间:2012/04/13