中国科学院机构知识库网格
Chinese Academy of Sciences Institutional Repositories Grid
机构
采集方式
内容类型
发表日期
学科主题
筛选

浏览/检索结果: 共4条,第1-4条 帮助

条数/页: 排序方式:
Microstructure, mechanical and tribological properties of plasma-sprayed NiCrAlY-Mo-Ag coatings from conventional and nanostructured powders 期刊论文  OAI收割
Surface and Coatings Technology, 2017, 卷号: 324, 页码: 552-559
作者:  
Li B(李博);  Jia JH(贾均红);  Han MM(韩敏敏);  Gao, Yimin;  Wang WZ(王文珍)
  |  收藏  |  浏览/下载:46/0  |  提交时间:2017/11/24
Transparent and Dense Ladder-Like Alkylene-Bridged Polymethylsiloxane Coating with Enhanced Water Vapor Barrier Property 期刊论文  OAI收割
acs applied materials & interfaces, 2015, 卷号: 7, 期号: 40, 页码: 22157-22165
作者:  
Zhang, Ce;  Zhang, Cong;  Cui, Xinmin;  Sun, Jinghua;  Ding, Ruimin
收藏  |  浏览/下载:44/0  |  提交时间:2015/11/18
Vertical geometry ultraviolet photodetectors with high photosensitivity based on nanocrystalline TiO2 films 期刊论文  OAI收割
Thin Solid Films, 2012, 卷号: 520, 期号: 24, 页码: 7144-7146
W. F. Xiang; P. R. Yang; A. J. Wang; K. Zhao; H. Ni; S. X. Zhong
收藏  |  浏览/下载:23/0  |  提交时间:2013/02/05
Surface modification of SiC mirror by IARE method (EI CONFERENCE) 会议论文  OAI收割
7th International Conference on Thin Film Physics and Applications, September 24, 2010 - September 27, 2010, Shanghai, China
作者:  
Gao J.
收藏  |  浏览/下载:30/0  |  提交时间:2013/03/25
A method to prepare high quality SiC coating at low temperature using large aperture E-beam evaporation PVD equipment with ion assistance was developed for the surface modification of SiC mirror for space projects. This method was called Ion Assisted Reactive Evaporation (IARE). The modified SiC coating was prepared using CH4 and Si with Kaufman ion source by IARE at 300C and it had met the requirements of applications. The SiC coating prepared by this method was amorphous. It was dense  homogeneous and easy to be polished. The surface modification of a SiC mirror was carried out using SiC coating by this method and achieved a fine surface modification effect. The surface roughness (rms) of the SiC substrate was reduced to 0.862nm  the scattering coefficient was reduced to 2.79% and the reflectance coated with Ag film was improved simultaneously after the surface modification. The effect of surface modification using SiC coating was close to that of using Si coating. It can be drawn that this technological method to preparation SiC coating for the surface modification of SiC mirror is reasonable and effective. 2011 SPIE.