中国科学院机构知识库网格
Chinese Academy of Sciences Institutional Repositories Grid
首页
机构
成果
学者
登录
注册
登陆
×
验证码:
换一张
忘记密码?
记住我
×
校外用户登录
CAS IR Grid
机构
金属研究所 [4]
采集方式
OAI收割 [4]
内容类型
期刊论文 [4]
发表日期
2019 [2]
2012 [1]
2002 [1]
学科主题
筛选
浏览/检索结果:
共4条,第1-4条
帮助
条数/页:
5
10
15
20
25
30
35
40
45
50
55
60
65
70
75
80
85
90
95
100
排序方式:
请选择
提交时间升序
提交时间降序
题名升序
题名降序
作者升序
作者降序
发表日期升序
发表日期降序
Effect of Y content on interface reaction and wettability between a nickel-base single crystal superalloy melt and ceramic mould
期刊论文
OAI收割
JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 卷号: 789, 页码: 472-484
作者:
Zi, Yun
;
Meng, Jie
;
Zhang, Chaowei
;
Yang, Yanhong
;
Zhou, Yizhou
  |  
收藏
  |  
浏览/下载:17/0
  |  
提交时间:2021/02/02
Nickel-base single crystal superalloy melt
Ceramic mould
Interface reaction
Wettability
Y content
Effect of Y content on interface reaction and wettability between a nickel-base single crystal superalloy melt and ceramic mould
期刊论文
OAI收割
JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 卷号: 789, 页码: 472-484
作者:
Zi, Yun
;
Meng, Jie
;
Zhang, Chaowei
;
Yang, Yanhong
;
Zhou, Yizhou
  |  
收藏
  |  
浏览/下载:16/0
  |  
提交时间:2021/02/02
Nickel-base single crystal superalloy melt
Ceramic mould
Interface reaction
Wettability
Y content
Mechanism of competitive growth during directional solidification of a nickel-base superalloy in a three-dimensional reference frame
期刊论文
OAI收割
Acta Materialia, 2012, 卷号: 60, 期号: 9, 页码: 3965-3975
X. B. Meng
;
Q. Lu
;
X. L. Zhang
;
J. G. Li
;
Z. Q. Chen
;
Y. H. Wang
;
Y. Z. Zhou
;
T. Jin
;
X. F. Sun
;
Z. Q. Hu
收藏
  |  
浏览/下载:14/0
  |  
提交时间:2013/02/05
Directional solidification
Competitive growth
Non-uniplanar case
3-D
reference frame
Rotation
single-crystal superalloys
low-angle boundaries
seed melt-back
grain
structures
prediction
orientation
castings
model
Effect of the melt treatment temperature on the melt structure and microstructure of a nickel based singale crystal superalloy
期刊论文
OAI收割
ACTA METALLURGICA SINICA, 2002, 卷号: 38, 期号: 9, 页码: 920-924
作者:
Wang, Z
;
Li, JG
;
Zhao, NR
;
Jin, T
;
Zhang, JH
  |  
收藏
  |  
浏览/下载:5/0
  |  
提交时间:2021/02/02
Ni based single crystal superalloy
melt structure
superheating treatment
solidified microstructure