条数/页: 排序方式:
The creep deformation mechanisms of a newly designed nickel-base superalloy 期刊论文  OAI收割
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 卷号: 710, 页码: 309-317
作者:  
Cui, LQ;  Yu, JJ;  Liu, JL;  Jin, T;  Sun, XF
  |  收藏  |  浏览/下载:50/0  |  提交时间:2018/06/05
The deformation and the recrystallization initiation in the dendrite core and interdendritic regions of a directionally solidified nickel-based superalloy 期刊论文  OAI收割
Journal of Alloys and Compounds, 2015, 卷号: 629, 页码: 247-254
L.; Jiang Wang, W. G.; Lou, L. H.
收藏  |  浏览/下载:23/0  |  提交时间:2015/05/08
Corporate Effects of Temperature and Strain Range on the Low Cycle Fatigue Life of a Single-Crystal Superalloy DD10 期刊论文  OAI收割
Acta Metallurgica Sinica-English Letters, 2015, 卷号: 28, 期号: 2, 页码: 152-158
Z. D.; Wang Fan, D.; Lou, L. H.
收藏  |  浏览/下载:27/0  |  提交时间:2015/05/08
EFFECT OF LATERAL PRE-COMPRESSION ON CREEP BEHAVIOR OF A 011 ORIENTED SINGLE CRYSTAL NICKEL-BASED SUPERALLOY 期刊论文  OAI收割
ACTA METALLURGICA SINICA, 2015, 卷号: 51, 期号: 5, 页码: 612-622
作者:  
Su Yong;  Tian Sugui;  Yu Huichen;  Yu Lili
  |  收藏  |  浏览/下载:22/0  |  提交时间:2021/02/02
Creep property and microstructure evolution of a nickel-base single crystal superalloy in 011 orientation 期刊论文  OAI收割
Materials Characterization, 2013, 卷号: 86, 页码: 177-184
G. M. Han; J. J. Yu; Z. Q. Hu; X. F. Sun
收藏  |  浏览/下载:44/0  |  提交时间:2014/02/19
The effect of reheat treatments on recovering the creep behavior of a corrosion-resistant nickel-based superalloy 期刊论文  OAI收割
Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2013, 卷号: 560, 页码: 25-33
J. S. Hou; L. Z. Zhou; C. Yuan; Z. Tang; J. T. Guo; X. Z. Qin; P. K. Liaw
收藏  |  浏览/下载:39/0  |  提交时间:2013/12/24
Effect of Threshold Stress on Anisotropic Creep Properties of Single Crystal Nickel-Base Superalloy SRR99 期刊论文  OAI收割
Journal of Materials Science & Technology, 2012, 卷号: 28, 期号: 5, 页码: 439-445
G. M. Han; J. J. Yu; X. F. Sun; Z. Q. Hu
收藏  |  浏览/下载:22/0  |  提交时间:2013/02/05
Influence of the characteristic of recrystallization grain boundary on the formation of creep cracks in a directionally solidified Ni-base superalloy 期刊论文  OAI收割
Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2012, 卷号: 532, 页码: 579-584
G. Xie; L. H. Lou
收藏  |  浏览/下载:23/0  |  提交时间:2013/02/05
Orientation Dependence of Stress Rupture Properties of a Ni-based Single Crystal Superalloy at 760 degrees C 期刊论文  OAI收割
Journal of Materials Science & Technology, 2012, 卷号: 28, 期号: 3, 页码: 229-233
S. H. Zhang; D. Wang; J. Zhang; L. H. Lou
收藏  |  浏览/下载:22/0  |  提交时间:2013/02/05
Intermediate temperature creep of directionally solidified Ni-based superalloy containing local recrystallization 期刊论文  OAI收割
Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2011, 卷号: 528, 期号: 7-8, 页码: 3062-3068
G. Xie; L. Wang; J. Zhang; L. H. Lou
收藏  |  浏览/下载:20/0  |  提交时间:2012/04/13