Effect of P and B compound strengthening on the evolution of phases and stress rupture properties of the IN718 superalloy during long-term aging at 650 & DEG;C 期刊论文  OAI收割
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 卷号: 881, 页码: 14
作者:  
Wang, Zhiyuan;  Zhang, Weiwei;  Li, Shaowei;  Mei, Feiqiang;  Xin, Xin
  |  收藏  |  浏览/下载:26/0  |  提交时间:2024/01/08
Re-recognition of the Effects of Phosphorus and Boron on the gamma '' and gamma ' Phases in IN718 Alloy 期刊论文  OAI收割
ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2019, 卷号: 32, 期号: 3, 页码: 372-380
作者:  
Zhang, An-Wen;  Li, Yang;  Zhang, Sha;  Liu, Fang;  Zhang, Wei-Hong
  |  收藏  |  浏览/下载:26/0  |  提交时间:2021/02/02
Residual Stress Evolution and Its Mechanism During the Manufacture of Superalloy Disk Forgings 期刊论文  OAI收割
ACTA METALLURGICA SINICA, 2019, 卷号: 55, 期号: 9, 页码: 1160-1174
作者:  
Bi Zhongnan;  Qin Hailong;  Dong Zhiguo;  Wang Xiangping;  Wang Ming
  |  收藏  |  浏览/下载:34/0  |  提交时间:2021/02/02
Re-recognition of the Effects of Phosphorus and Boron on the γ'' and γ' Phases in IN718 Alloy 期刊论文  OAI收割
Acta Metallurgica Sinica(English Letters), 2019, 卷号: 32, 期号: 3, 页码: 372-380
作者:  
Zhang Anwen;  Li Yang;  Zhang Sha;  Liu Fang;  Zhang Weihong
  |  收藏  |  浏览/下载:27/0  |  提交时间:2021/02/02
Re-recognition of the Effects of Phosphorus and Boron on the γ'' and γ' Phases in IN718 Alloy 期刊论文  OAI收割
Acta Metallurgica Sinica(English Letters), 2019, 卷号: 32, 期号: 3, 页码: 372-380
作者:  
Zhang Anwen;  Li Yang;  Zhang Sha;  Liu Fang;  Zhang Weihong
  |  收藏  |  浏览/下载:26/0  |  提交时间:2021/02/02
Refinement Mechanism of Low Voltage Pulsed Magnetic Field on Solidification Structure of Silicon Steel 期刊论文  OAI收割
Metals and Materials International, 2014, 卷号: 20, 期号: 3, 页码: 527-530
Y. J. Li; Y. F. Teng; Y. S. Yang
收藏  |  浏览/下载:95/0  |  提交时间:2015/01/14
Grain refinement of as cast superalloy K4169 solidified with low voltage pulsed magnetic field 期刊论文  OAI收割
Materials Research Innovations, 2014, 卷号: 18, 页码: 352-356
Y. F.; Feng Teng, X. H.; Li, Y. J.; Yang, Y. S.
收藏  |  浏览/下载:94/0  |  提交时间:2015/05/08
Hot die forging process optimization of superalloy IN718 turbine disc using processing map and finite element method 期刊论文  OAI收割
Proceedings of the Institution of Mechanical Engineers Part B-Journal of Engineering Manufacture, 2010, 卷号: 224, 期号: B1, 页码: 103-110
H. Y. Zhang; S. H. Zhang; Z. X. Li; M. Cheng
收藏  |  浏览/下载:29/0  |  提交时间:2012/04/13
Effect of temperature and strain amplitude on dislocation structure of M963 superalloy during high-temperature low cycle fatigue 期刊论文  OAI收割
Materials Transactions, 2006, 卷号: 47, 期号: 1, 页码: 67-71
L. Z. He; Q. Zheng; X. F. Sun; H. R. Guan; Z. Q. Hu; K. Tieu; C. Lu; H. T. Zhu
收藏  |  浏览/下载:30/0  |  提交时间:2012/04/13
Processing and microstructural evolution of superalloy inconel 718 during hot tube extrusion 期刊论文  OAI收割
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2005, 卷号: 21, 期号: 2, 页码: 175-178
作者:  
Zhang, SH;  Wang, ZT;  Qiao, B;  Xu, Y;  Xu, TF
  |  收藏  |  浏览/下载:10/0  |  提交时间:2021/02/02