中国科学院机构知识库网格
Chinese Academy of Sciences Institutional Repositories Grid
首页
机构
成果
学者
登录
注册
登陆
×
验证码:
换一张
忘记密码?
记住我
×
校外用户登录
CAS IR Grid
机构
金属研究所 [11]
合肥物质科学研究院 [1]
采集方式
OAI收割 [12]
内容类型
期刊论文 [12]
发表日期
2020 [1]
2019 [1]
2018 [2]
2017 [1]
2014 [1]
2012 [1]
更多
学科主题
Materials ... [2]
Engineerin... [1]
Metallurgy... [1]
Nanoscienc... [1]
筛选
浏览/检索结果:
共12条,第1-10条
帮助
条数/页:
5
10
15
20
25
30
35
40
45
50
55
60
65
70
75
80
85
90
95
100
排序方式:
请选择
提交时间升序
提交时间降序
作者升序
作者降序
题名升序
题名降序
发表日期升序
发表日期降序
Effect of strain rate on plastic deformation bonding behavior of Ni-based superalloys
期刊论文
OAI收割
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2020, 卷号: 40, 页码: 54-63
作者:
Zhang, Jian Yang
;
Xu, Bin
;
Tariq, Naeem ul Haq
;
Sun, Ming Yue
;
Li, Dian Zhong
  |  
收藏
  |  
浏览/下载:27/0
  |  
提交时间:2021/02/02
Inconel 718 superalloy
Isothermal compression bonding
Dynamic recrystallization
Grain boundary
Subgrain
Strain rate
Residual Stress Evolution and Its Mechanism During the Manufacture of Superalloy Disk Forgings
期刊论文
OAI收割
ACTA METALLURGICA SINICA, 2019, 卷号: 55, 期号: 9, 页码: 1160-1174
作者:
Bi Zhongnan
;
Qin Hailong
;
Dong Zhiguo
;
Wang Xiangping
;
Wang Ming
  |  
收藏
  |  
浏览/下载:36/0
  |  
提交时间:2021/02/02
TEMPERATURE STRUCTURE STABILITY
SITU NEUTRON-DIFFRACTION
IN-SITU
SINGLE-CRYSTAL
CREEP-BEHAVIOR
TURBINE DISC
INCONEL 718
RELAXATION
MICROSTRUCTURE
DISTORTION
superalloy
residual stress
neutron diffraction
contour method
turbine disk
Tool wear performance and surface integrity studies for milling DD5 Ni-based single crystal superalloy
期刊论文
OAI收割
SCIENCE CHINA-TECHNOLOGICAL SCIENCES, 2018, 卷号: 61, 期号: 4, 页码: 522-534
作者:
Gong, YD
;
Li, Q
;
Li, JG
;
Liu, Y
;
Sun, Y
  |  
收藏
  |  
浏览/下载:29/0
  |  
提交时间:2018/06/05
Minimum Quantity Lubrication
Nickel-based Superalloy
Inconel 718
Cutting Forces
Alloys
Dry
Mechanisms
Life
Grinding temperature and power consumption in high speed grinding of Inconel 718 nickel-based superalloy with a vitrified CBN wheel
期刊论文
OAI收割
PRECISION ENGINEERING-JOURNAL OF THE INTERNATIONAL SOCIETIES FOR PRECISION ENGINEERING AND NANOTECHNOLOGY, 2018, 卷号: 52, 期号: 无, 页码: 192-200
作者:
Dai, Chen-Wei
;
Ding, Wen-Feng
;
Zhu, Ye-Jun
;
Xu, Jiu-Hua
;
Yu, Hai-Wu
  |  
收藏
  |  
浏览/下载:38/0
  |  
提交时间:2019/11/11
High speed grinding
Vitrified CBN wheel
Inconel 718 nickel-based superalloy
Grinding temperature
Power consumption
Preparation of hot-isostatic-pressed powder metallurgy superalloy Inconel 718 free of prior particle boundaries
期刊论文
OAI收割
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 卷号: 682, 页码: 341-344
Chang, Litao
;
Sun, Wenru
;
Cui, Yuyou
;
Yang, Rui
收藏
  |  
浏览/下载:52/0
  |  
提交时间:2017/08/17
Superalloy
Powder metallurgy
Hot isostatic pressing
Prior particle boundary
Inconel 718
Effect of heat treatment on microstructure and mechanical properties of the hot-isostatic-pressed Inconel 718 powder compact
期刊论文
OAI收割
Journal of Alloys and Compounds, 2014, 卷号: 590, 页码: 227-232
L. T. Chang
;
W. R. Sun
;
Y. Y. Cui
;
F. Q. Zhang
;
R. Yang
收藏
  |  
浏览/下载:27/0
  |  
提交时间:2014/03/14
Superalloy
Inconel 718
Hot isostatic pressing
Heat treatment
gamma
'' precipitation
Ductility
superalloy inconel-718
precipitation
alloy
Influence of deformation level on microstructure and creep behavior of GH4169 alloy
期刊论文
OAI收割
Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2012, 卷号: 550, 页码: 235-242
S. G. Tian
;
Z. R. Li
;
Z. G. Zhao
;
L. Q. Chen
;
W. R. Sun
;
X. H. Liu
收藏
  |  
浏览/下载:30/0
  |  
提交时间:2013/02/05
GH4169 alloy
Hot continuous rolling
Microstructure
Creep
Deformation
mechanism
intermediate temperature
inconel 718
superalloy
mechanisms
Segregation and diffusion behavior of niobium in a highly alloyed nickel-base superalloy
期刊论文
OAI收割
Transactions of Nonferrous Metals Society of China, 2011, 卷号: 21, 期号: 11, 页码: 2402-2407
X. L. Pan
;
H. Y. Yu
;
G. F. Tu
;
W. R. Sun
;
Z. Q. Hu
收藏
  |  
浏览/下载:33/0
  |  
提交时间:2012/04/13
GH742y superalloy
niobium
segregation
diffusion
directionally solidified superalloy
inconel-718 alloy
microstructure
homogenization
gamma'
Hot die forging process optimization of superalloy IN718 turbine disc using processing map and finite element method
期刊论文
OAI收割
Proceedings of the Institution of Mechanical Engineers Part B-Journal of Engineering Manufacture, 2010, 卷号: 224, 期号: B1, 页码: 103-110
H. Y. Zhang
;
S. H. Zhang
;
Z. X. Li
;
M. Cheng
收藏
  |  
浏览/下载:30/0
  |  
提交时间:2012/04/13
superalloy IN718
turbine disc
processing map
finite element method
microstructure simulation
high-temperature deformation
metadynamic recrystallization
microstructural evolution
flow behavior
inconel-718
working
simulation
in-718
High temperature low cycle fatigue behavior of a directionally solidified Ni-base superalloy DZ951
期刊论文
OAI收割
Materials Science and Engineering a-Structural Materials Properties Microstructure and Processing, 2008, 卷号: 488, 期号: 1-2, 页码: 389-397
Z. K. Chu
;
J. J. Yu
;
X. F. Sun
;
H. R. Guan
;
Z. Q. Hu
收藏
  |  
浏览/下载:37/0
  |  
提交时间:2012/04/13
nickel-base superalloy
low cycle fatigue
cyclic deformation
cyclic
stress response
nimonic pe-16 superalloy
room-temperature
crystallographic
orientation
inconel 718
strain-rate
deformation
mechanisms
property
fracture
tensile